Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 200 - 500 µm | 200 - 500 µm | |
Polimeri Europa Extir® F 1111 Expandable Polystyrene
(discontinued **) Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont.. |
|||
Particle Size | 200 - 500 µm | 200 - 500 µm | |
Polimeri Europa Extir® P 1212 Expandable Polystyrene
(discontinued **) Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. .. |
|||
Particle Size | 125 - 500 µm | 125 - 500 µm | Average value: 283 µm Grade Count:3 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Particle Size | 200 - 500 µm | 200 - 500 µm | GB/T 12005.7 |
Lushan DE-1 Polyethylene Sintered Powder PE sintered powder Lushan DE-1 is combined with more than 10 years practice and experience on the area of oil & gas pipeline anti-corrosion. PE sintered powder Lushan DE-1 is used on anti-corrosion .. |
|||
Particle Size | 200 - 500 µm | 200 - 500 µm | GB/T 12005.7 |
Lushan DP-1 Polypropylene sintered powder, Ultra Fast Cure PP sintered powder Lushan DP-1 is used on anti-corrosion coated steel pipe Polypropylene top coats and applied in oil & gas submarine counterweight pipeline to make a non-slid surface to avoid skidd.. |
|||
Particle Size | 200 - 500 µm | 200 - 500 µm | Dry |
Shamrock Technologies NanoFLON® P 39B Thermoplastic Grade PTFE Additive Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro.. |
|||
Particle Size | 200 - 500 µm | 200 - 500 µm | Dry |
Shamrock Technologies NanoFLON® P 40A Thermoplastic Grade PTFE Additive Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro.. |
|||
Particle Size | 200 - 500 µm | 200 - 500 µm | Dry |
Shamrock Technologies NanoFLON® P 47A Thermoplastic Grade PTFE Additive Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro.. |
|||
Particle Size | 200 - 500 µm | 200 - 500 µm | Dry |
Shamrock Technologies NanoFLON® P 63B Thermoplastic Grade PTFE Additive Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro.. |
|||
Particle Size | 10 - 500 µm | 10 - 500 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Particle Size | 10 - 500 µm | 10 - 500 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ HA Hollow Spheres EXTENDOSPHERESâ„¢ HA are off white, low-cost, low-density, high alumina, ceramic hollow spheres.Applications: Hollow spheres are ideal for use in coatings, sealants, caulks and other applications.. |
|||
Particle Size | 10 - 500 µm | 10 - 500 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ SG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Particle Size | 200 - 500 µm | 200 - 500 µm | Dry |
Shamrock Technologies NanoFLON® P 51A Thermoplastic Grade PTFE Additive Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro.. |
|||
Particle Size | 5.0 - 500 µm | 5.0 - 500 µm | |
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Particle Size | 5.0 - 500 µm | 5.0 - 500 µm | |
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Particle Size | 10 - 500 µm | 10 - 500 µm | |
Solvay MIRAPOL® SURF-S PFREE POWER Surfactant Description: Blend of acrylic based polymer and sodium carbonate. This polymer is used as a rinse-aid agent to replace the nonionic surfactant 3-in-1 product in automatic dish wash. It is very effic.. |