Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2000 - 3000 µm | 2000 - 3000 µm | Diameter per caliper rule |
Stanelco Bioplast® GS 2189 Biodegradable Plastic Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i.. |
|||
Particle Size | 1000 - 3000 µm | 1000 - 3000 µm | Diameter per caliper rule |
Stanelco Bioplast® Wrap 100 Biodegradable Plastic Bioplast Wrap 100 is a plasticiser-free thermoplastic material which allows the production of films with coated paper-like properties. Wrap 100 is an excellent, eco-friendly alternative to laminated.. |