Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 13.2 - 24 µm | 13.2 - 24 µm | d50 |
Indium Corp. Standard ITO Indium Tin Oxide Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo.. |
|||
Particle Size | 18 - 24 µm | 18 - 24 µm | 50% |
H.C. Starck Amperit® 588.059 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |
|||
Particle Size | 20 - 24 µm | 20 - 24 µm | 10% |
H.C. Starck Amperit® 109.066 Agglomerated Sintered Molybdenum (Mo) |
|||
Particle Size | 22 - 24 µm | 22 - 24 µm | D50 |
Sinotek Materials ZSG-23 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Particle Size | 16 - 24 µm | 16 - 24 µm | For Median |
CIMBAR Crescent 35 Calcium Carbonate (CaCO3), Medium Powder CIMBAR's Crescent product line is a natural calcium carbonate ground to various particle size distributions. The crystalline structure of the calcium carbonate in Crescent products has a predominan.. |
|||
Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
Akzo Nobel Expancel® 009 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
Akzo Nobel Expancel® 091 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
Akzo Nobel Expancel® 551 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
Akzo Nobel Expancel® 551 WU 80 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 16 - 24 µm | 16 - 24 µm | D(0.5) |
Akzo Nobel Expancel® 820 SL 80 Unexpanded microspheres in aqueous dispersion Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
Akzo Nobel Expancel® 950 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
Akzo Nobel Expancel® 092 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
Akzo Nobel Expancel® 091 WU 80 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 18 - 24 µm | 18 - 24 µm | 50% |
H.C. Starck Amperit® 529.053 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo) |
|||
Particle Size | 20 - 24 µm | 20 - 24 µm | 10% |
H.C. Starck Amperit® 584.1 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |