Particle Size 180 - 230 µm
180 - 230 µm
Median Granulate Size
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 180 - 230 µm
180 - 230 µm
Median Grain Diameter
Nabaltec GRANALOX® NM 9216 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 180 - 230 µm
180 - 230 µm
Median Grain Diameter
Nabaltec GRANALOX® NM 9612 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 180 - 230 µm
180 - 230 µm
Median Grain Diameter
Nabaltec GRANALOX® NM 9620 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 170 - 230 µm
170 - 230 µm
Mean Granulate Size
Nabaltec GRANALOX® NM 9622 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Particle Size 180 - 230 µm
180 - 230 µm
Median Grain Diameter
Nabaltec GRANALOX® NM 9622 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 180 - 230 µm
180 - 230 µm
Median Grain Diameter
Nabaltec GRANALOX® NM 9816 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 180 - 230 µm
180 - 230 µm
Median Grain Diameter
Nabaltec GRANALOX® NM 9923 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 110 - 230 µm
110 - 230 µm
Lucite International Elvacite ® 2021 Acrylic Resin
Elvacite® 2021 is a high molecular weight methyl methacrylate polymer. It is used in barrier coatings for vinyl. Its high molecular weight provides excellent abrasion resistance.Information provide..
Copyright © lookpolymers.com All Rights Reserved