Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 5.0 - 175 µm | 5.0 - 175 µm | range |
Potters Industries Q-Cel® 6019 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1221 High gloss PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1249 Sanitary, mix color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1841 Metallic colors Adding metallic effect pigments to powder coatings gave rise to several application problems such as “spitting”. Synres-Almoco’s Metallic PiMC 1841 ensures easy processing and homogeneous surface.. |
|||
Particle Size | 100 - 175 µm | 100 - 175 µm | D 0.9, SATP-114, Malvern method |
Raschig Group PiMC 1949 Granite colors PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |