Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 5.0 - 135 µm | 5.0 - 135 µm | |
Potters Industries Q-Cel® 7023S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 110 - 135 µm | 110 - 135 µm | Laser Light Scattering Method; LSY-QB-ID016 |
LG Chemical Lutex 105 NBR Latex Description: Tensile strength, Elongation, Oil resistance, Abrasion resistance, Softness, WhitenessApplication: Nitrile Glove (Examination Glove, Clean Room Glove), Supported Glove (Industrial Glove.. |
|||
Particle Size | 105 - 135 µm | 105 - 135 µm | Laser Light Scattering Method; LSY-QB-ID016 |
LG Chemical Lutex 703 SBR Latex Description: Binding Force, Ink set off, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Pre-Rod, Blade Coater, Adhesive coated paper and Carpet back-coating .. |
|||
Particle Size | 115 - 135 µm | 115 - 135 µm | Laser Light Scattering Method; LSY-QB-ID016 |
LG Chemical Lutex 810 SBR Latex Description: Blister Resistance, Ink set off, Sheet Gloss, Coater RunnabilityApplication: Art Paper, Web Offset, Blade Coater and Adhesive coated paperCSA No. 70857-13-5 and 7732-18-5Information pro.. |
|||
Particle Size | 115 - 135 µm | 115 - 135 µm | Laser Light Scattering Method; LSY-QB-ID016 |
LG Chemical Lutex M710 SBR Latex Description: High Binding Force (MSP), Ink set off, Print Mottle, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Top-Film Coater, Adhesive coated paper and Carpet back-coating adhesive.. |