Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 70 - 120 µm | 70 - 120 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9510 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 80 - 120 µm | 80 - 120 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 70 - 120 µm | 70 - 120 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9634 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 80 - 120 µm | 80 - 120 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9916 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 60 - 120 µm | 60 - 120 µm | mesh. |
Oceanchem Group Xanthan Gum Oil Drilling Grade Information Provided by Oceanchem Group |
|||
Particle Size | 5.0 - 120 µm | 5.0 - 120 µm | |
Potters Industries Q-Cel® 7028 Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |