Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.040 - 0.060 µm | 0.040 - 0.060 µm | outside diameter |
NanoAmor 95%, OD/L: 40-60 nm/1-2 um Multi-Walled Carbon Nanotubes |
|||
Particle Size | 0.040 - 0.060 µm | 0.040 - 0.060 µm | outside diameter |
NanoAmor 99%, OD/L: 40-60 nm/1-2 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.040 - 0.060 µm | 0.040 - 0.060 µm | outside diameter |
NanoAmor 95%, OD/ID: 40-60/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.060 µm | 0.020 - 0.060 µm | |
American Elements Beryllium Nanoparticles General DescriptionBeryllium (Be) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Beryllium Particles are typically 20-60 nanometers (nm) with specif.. |
|||
Particle Size | 0.020 - 0.060 µm | 0.020 - 0.060 µm | |
American Elements Magnesium Nanoparticles General DescriptionMagnesium (Mg) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Magnesium Particles are typically 20-60 nanometers (nm) with specif.. |
|||
Particle Size | 0.020 - 0.060 µm | 0.020 - 0.060 µm | |
American Elements Cobalt Nanoparticles General DescriptionCobalt (Co) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Cobalt Particles are typically 20-60 nanometers (nm) with specific sur.. |