Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 9.0 µm | <= 9.0 µm | 90% smaller than |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Particle Size | 9.0 µm | 9.0 µm | median; Microtrac |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | 9.0 µm | 9.0 µm | median; Microtrac |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | <= 9.0 µm | <= 9.0 µm | Average; Internal Method |
Solvay Specialty Polymers Algoflon® L206 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L206 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It is specially recommended for use as an additive in elastomers (e.g. perfluoroelastomers) t.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 9.0 - 11 µm | 9.0 - 11 µm | Average |
Malvern Minerals Trikup® PM Silane Treated Aluminum Hydroxide Trikup® is a custom, silane treated alumina trihydrate or aluminum hydroxide. ATH is the largest volume flame retardant in the world. Trikup® adds additional functionality through the use of .. |
|||
Particle Size | 9.0 µm | 9.0 µm | 90% |
Minelco UltraCarb LH15C-10 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 90% |
Minelco UltraCarb LH15X Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 9.0 - 12 µm | 9.0 - 12 µm | Mean particle size is 9 to 12 µm. Crystal size is >10 µm. %-325 mesh is 99.9%. |
Momentive Performance Materials AC-6004 Boron Nitride (BN) Powder Grade AC-6004 is a high purity, fine (99%,-325 mesh) Boron Nitride (BN) powder with a hexagonal crystal structure and large graphite-like platelets. It exhibits the unique properties of boron nitri.. |
|||
Particle Size | 9.0 µm | 9.0 µm | Mean |
Momentive Performance Materials AC6069 Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powder grade AC6069 consists of single-crystal hexagonal particles with an average particle size of 9 µm. AC6069 has a relatively tight particle size distr.. |
|||
Particle Size | 9.0 - 13 µm | 9.0 - 13 µm | |
H.C. Starck Amperit® 140.067 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 9.0 µm | 9.0 µm | |
Silberline A-6578FG A-6578FG is a standard polished grade; class A, fine leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance |
|||
Particle Size | 9.0 µm | 9.0 µm | |
Silberline L-2422-PA L-2422PA is a small particle size, bright leafing aluminum pigment based on standard cornflake geometry. It is a cost effective pigment for producing strong metallic effects with good coverage in li.. |
|||
Particle Size | 9.0 µm | 9.0 µm | Before Conversion |
Silberline Silvet® 220-20-E Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatible with.. |
|||
Particle Size | 9.0 µm | 9.0 µm | Before Conversion |
Silberline Silvet® 220-30-E1 Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final processi.. |
|||
Particle Size | 9.0 µm | 9.0 µm | |
Silberline "A" Series A-1592FG A-1592FG is a very fine, high opacity, non-leafing aluminum pigment for solvent based industrial coatings. Due to the small particle size, this grade is well suited for imparting high opacity at low.. |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | d90, Guaranteed |
TIMCAL TIMREX® LSG10 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 9.0 - 15.5 µm | 9.0 - 15.5 µm | d90, Guaranteed |
TIMCAL TIMREX® SFG10 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 9.0 µm | 9.0 µm | Median |
CIMBAR EliteTalc® 21 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |
|||
Particle Size | 9.0 - 12 µm | 9.0 - 12 µm | D50 |
CIMBAR UltraMag & UltraMag ST 10 Magnesium Hydroxide Powder UltraMag is a naturally ground, white, high-purity Magnesium Hydroxide suitable for a wide range of applications including water treatment slurries, plastics, rubber and flame-retardant/smoke suppre.. |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | D(0.5) |
Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | D(0.5) |
Akzo Nobel Expancel® 461 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | D(0.5) |
Akzo Nobel Expancel® 461 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 9.0 µm | 9.0 µm | Median |
World Minerals Celite® White Mist® PF Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 90" Percentile |
3M W-210 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Particle Size | <= 9.0 µm | <= 9.0 µm | average |
Oceanchem Group Magnesium Hydroxide Molecular Formula: Mg(OH)2Cas No.: 1309-42-8Use: Magnesium hydroxide is a non-halogen flame retardant recommended where use of halogenated products is limited or prohibited. In addition, it is an e.. |
|||
Particle Size | 9.0 µm | 9.0 µm | |
Asahi Glass Fluon® L150J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |