Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 80 µm | <= 80 µm | 90% smaller than |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 80 - 120 µm | 80 - 120 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 80 - 120 µm | 80 - 120 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9916 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 80 µm | 80 µm | Mean |
Potters Industries Q-Cel® 7019 Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 80 µm | 80 µm | Method C; ASTM D1921 |
Solvay Specialty Polymers Halar® 6014 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)&l Halar® 6014 is a clear, semi-crystalline melt processable fluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in protection and .. |
|||
Particle Size | 80 µm | 80 µm | Method C; ASTM D1921 |
Solvay Specialty Polymers Halar® 6014F Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Halar® 6014F is a clear, semi-crystalline melt processable fluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in protection and.. |
|||
Particle Size | 80 µm | 80 µm | Method C; ASTM D1921 |
Solvay Specialty Polymers Halar® 6914 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)&l Halar® 6914 is a gray, semi-crystalline melt processable fluorinated primer. It is designed to be applied directly to substrates by electrostatic or fluidized bed techniques. In particular Halar® .. |
|||
Particle Size | 80 µm | 80 µm | |
Gromax EP-5016M Unplasticized Vinyl Acetate homopolymer Product Description: EP-5016M is a water redispersible vinyl acetate homopolymer powder that is readily dispersible in water and forms stable emulsion. This redispersible powder is especially recomm.. |
|||
Particle Size | 80 - 100 µm | 80 - 100 µm | |
Lucite International Colacryl ® DP300 Specialty Acrylic Resin This is a high molecular weight PMMA resin. PMMA resins are characterised by high physical strength and abrasion resistance.Applications:This resin is used in the production of porous polymer molds .. |
|||
Particle Size | 80 - 100 µm | 80 - 100 µm | |
Lucite International Colacryl ® DP300S Acrylic Dental Resin Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties... |
|||
Particle Size | 80 - 100 µm | 80 - 100 µm | |
Lucite International Colacryl ® DP300S Specialty Acrylic Resin Colacryl® DP 300S has been designed for use as a dental polymer. Typical applications for this product include formulated, acrylic tooth polymer for manufacture of artificial teeth and denture ba.. |
|||
Particle Size | <= 80 µm | <= 80 µm | > 99 wt.%; DIN EN ISO 4610 |
Suzhou Hipro Polymers Hiprolon® 11 PES Colorized Nylon powder Hiprolon® 11 PES colorized electrostatic polyamide powder is partly comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resist.. |
|||
Particle Size | <= 80 µm | <= 80 µm | > 99 wt.%; DIN EN ISO 4610 |
Suzhou Hipro Polymers Hiprolon® 211 PES Colorized Nylon powder Hiprolon® 211 PES colorized electrostatic polyamide powder is fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resist.. |
|||
Particle Size | 80 µm | 80 µm | |
TIMCAL TIMREX® M80 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 80 µm | 80 µm | at a density of 1.48 g/cc, pressure of 2.5 t/cc |
TIMCAL TIMREX® T44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | <= 80 µm | <= 80 µm | Top Size |
Excalibar NewBar™ API Barite BaSO4 Powder NewBar™ API barite product is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas explorati.. |
|||
Particle Size | <= 80 µm | <= 80 µm | Top Size |
Excalibar NewWate™ Barite BaSO4 Powder NewWate™ barite is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas exploration. NewWate.. |
|||
Particle Size | 80 µm | 80 µm | 90th% |
3M K37 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 80 µm | 80 µm | Effective Top Size |
3M K46 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 80 µm | 80 µm | Effective Top Size |
3M S32 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 80 µm | 80 µm | Effective Top Size |
3M S35 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | <= 80 µm | <= 80 µm | 90% smaller than |
Nyco ULTRAFIBRE® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 80 µm | 80 µm | 95th% |
3M D32/4500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 80 µm | 80 µm | Method C; ASTM D1921 |
Solvay Specialty Polymers Halar® 6514 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)&l Halar 6514 is a black, semi-crystalline melt processable fluorinated primer. It is designed to be applied directly to substrates by electrostatic or fluidized bed techniques. In particular Halar 651.. |
|||
Particle Size | 80 µm | 80 µm | Method C; ASTM D1921 |
Solvay Specialty Polymers Halar® 6614 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)&l Halar® 6614 is a green, semi-crystalline melt processable fluorinated primer. It is designed to be applied directly to substrates by electrostatic or fluidized bed techniques. In particular Halar®.. |
|||
Particle Size | 80 µm | 80 µm | Before Conversion |
Silberline Sparkle Silvet® 764-30-E1 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final pr.. |