Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 75 µm | 75 µm | mean value |
Potters Industries Q-Cel® 6019 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro EG 2018 Display Device Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and .. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro EG 2020 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 750 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | <= 75 µm | <= 75 µm | REG Powder |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 75 µm | <= 75 µm | REG Powder |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | <= 75 µm | <= 75 µm | REG Powder |
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Particle Size | 75 µm | 75 µm | Maximum of 5% greater than, Ni-SF RC 60 |
H.C. Starck Amperit® 568.005 Tungsten Carbide-Nickel 92-8 - Nickel SF RC 60 65-35 Composition is of NiSF RC 60 only |
|||
Particle Size | 75 µm | 75 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 599.063 Agglomerated Sintered Molybdenum Carbide (Cr2O3) |
|||
Particle Size | 75 - 105 µm | 75 - 105 µm | |
Lucite International Lucite® 41 Acrylic Resin for Casting and Embedments Lucite® 41 is a high molecular weight methyl methacrylate homopolymer for use in castings & embedments.Like all Lucite® Acrylic Resins for castings & embedments, Lucite® 41 offers: Exceptio.. |
|||
Particle Size | 75 - 105 µm | 75 - 105 µm | |
Lucite International Lucite® 6751 Acrylic Bead Resin Lucite® acrylic resins are used in a variety of industrial, commercial and architectural applications. They’re a favorite among manufacturers of commemorative embedments because of their exc.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | <= 75 µm | <= 75 µm | Scattered Fineness |
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder Conformable with: Q/DYS 014-2007Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resist.. |
|||
Particle Size | <= 75 µm | <= 75 µm | <5%; TI-2087 |
Solvay RHODOPOL® TG Surfactant Description: Transparent, granular grade xanthan gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent.Identification: XANTHAN GUMCAS: 11138 – 66 – .. |
|||
Particle Size | 75 µm | 75 µm | at a density of 1.73 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | Springback 20.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | at a density of 1.73 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® KS44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | Springback 17%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS5-25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | Springback 17%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS5-44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | at a density of 2.03 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | Springback 6.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® SFG150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | at a density of 2.03 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | at a density of 2.03 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | <= 75 µm | <= 75 µm | < 3.0 wt% above |
Excalibar NewWate™ Barite BaSO4 Powder NewWate™ barite is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas exploration. NewWate.. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro CF 7570 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific ther.. |
|||
Particle Size | <= 75 µm | <= 75 µm | VSD Powder |
Ferro CF 7572 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci.. |