Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 70 µm | 70 µm | median; Microtrac |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 70 - 120 µm | 70 - 120 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9510 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 70 - 120 µm | 70 - 120 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9634 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 70 µm | 70 µm | Mean |
Potters Industries Q-Cel® 6019S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 70 µm | 70 µm | mean value |
Potters Industries Q-Cel® 6028 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Particle Size | 70 - 100 µm | 70 - 100 µm | Mean |
Potters Industries Spheriglass® 2429 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Size | 70 µm | 70 µm | Geon® 812 |
PolyOne Geon™ 210 Series 218 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol and or Fused Film Formulation F2 consists of 60 parts of Geon®178 + 40 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940 Note: Plastisol Formulation F1 consis.. |
|||
Particle Size | 70 µm | 70 µm | D<sub>50</sub>; ISO 13320-1 |
Victrex® PEEK 600PF Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact complian.. |
|||
Particle Size | <= 70 µm | <= 70 µm | d50 |
Magyar Aluminum ALO-Ex35 LS Alumina Calcined Alumina |
|||
Particle Size | 70 - 90 µm | 70 - 90 µm | Laser Light Scattering Method; LSY-QB-ID016 |
LG Chemical Lutex 760 SBR Latex Description: Binding Force, Print gloss, High Shear Rheology, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Top-Film, Blade Coater, Adhesive coated paper an.. |
|||
Particle Size | 70 µm | 70 µm | Before Conversion |
Silberline Silvet® 460-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Particle Size | 70 µm | 70 µm | d90 |
TIMCAL TIMREX® KS5-75TT Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 70 µm | 70 µm | at a density of 2.20 g/cc |
TIMCAL TIMREX® T150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 70 µm | 70 µm | at a density of 2.20 g/cc |
TIMCAL TIMREX® T15-75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 70 µm | 70 µm | at a density of 2.20 g/cc |
TIMCAL TIMREX® T200-2000 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 70 µm | 70 µm | at a density of 2.20 g/cm<sup>3</sup> |
TIMCAL TIMREX® T75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 70 µm | 70 µm | at a density of 2.20 g/cc |
TIMCAL TIMREX® T800 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 70 µm | 70 µm | TEC QSD |
Trelleborg AEM Eccospheres® SI-100 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Particle Size | 70 µm | 70 µm | at a density of 2.20 g/cc |
TIMCAL TIMREX® T150-600 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 70 µm | 70 µm | 95th% |
3M H50/10000EPX Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 70 µm | 70 µm | 90th% |
3M K46 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 70 µm | 70 µm | 90th% |
3M S32 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 70 µm | 70 µm | 90th% |
3M S38HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |