Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 7.5 µm | 7.5 µm | Median Diameter |
Omya OMYACARB® 8 - LU Calcium Carbonate A medium, dry ground calcium carbonate with a closely controlled particle size distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated.. |
|||
Particle Size | 7.5 µm | 7.5 µm | Median Diameter |
Omya PULPROWHITE® 8 - SA Calcium Carbonate A dry ground calcium carbonate with an intermediate and closely sized particle distribution.Information supplied by Omya North America. |
|||
Particle Size | 7.5 µm | 7.5 µm | 50% of particles, (REG Powder) |
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Particle Size | 7.5 µm | 7.5 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade AX 20 Silicon Metal Powder Si high purity min. 99.995%Raw material for reaction bonded silicon nitride (RBSN)Silicon metal infiltration for SiC (SiSiC) |
|||
Particle Size | 7.5 µm | 7.5 µm | median |
Esstech V-117-1075 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |
|||
Particle Size | 7.5 µm | 7.5 µm | Median |
World Minerals Celite® Super Floss® Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |