Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 43 - 57 µm | 43 - 57 µm | 90% |
H.C. Starck Amperit® 582.072 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Particle Size | 43 µm | 43 µm | d90 |
TIMCAL TIMREX® HSAG100 Primary Synthetic High Surface Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 43 µm | 43 µm | Springback 20.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 43 µm | 43 µm | Typical |
TIMCAL TIMREX® LSG 44 Natural Graphite Flakes TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 43 µm | 43 µm | springback 20.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® T150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 43 µm | 43 µm | springback 20.5%, pressure at 0.477 t/cc |
TIMCAL TIMREX® T15-75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 43 µm | 43 µm | springback 20.5%, pressure of 0.477 t/cc |
TIMCAL TIMREX® T44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 43 µm | 43 µm | springback 20.5%, pressure at 0.0477t/gg |
TIMCAL TIMREX® T75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 43 µm | 43 µm | d90, Typical |
TIMCAL TIMREX® C-LUB 310 Primary Synthetic Graphite Information provided by TIMCAL |