Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco 10 WOLLASTOCOAT® Wollastonite Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco M1250 AS WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | >= 4.0 µm | >= 4.0 µm | 10% smaller than |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco NYAD® M1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | 4.0 µm | 4.0 µm | Median Grain Diameter |
Nabaltec NABALOX® NO 115-25 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 4.0 µm | 4.0 µm | |
Poco Graphite DFP Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Particle Size | 4.0 µm | 4.0 µm | mean aggregate size |
NanoScale NanoActive® Zinc Oxide NanoActive ZnO is produced using proprietary processes to obtain high specific surface area, small crystallite size material that can be dispersed in various carrier fluids with significantly reduce.. |
|||
Particle Size | 4.0 µm | 4.0 µm | |
Poco Graphite DFP-3-2 Ion Implant Grade Graphite This is a high strength graphite that has reduced porosity. DFP-3-2 has long been the standard for components that exhibit long life and reduced erosion rates. |
|||
Particle Size | 4.0 µm | 4.0 µm | 10% finer than |
Potters Industries Sphericel® 110P8 Hollow Glass Spheres Description: Sphericel® 110P8 hollow glass spheres displace the same volume of resin as solid spheres of the same size, but are lighter. Using Sphericel® hollow glass spheres, plastics engineers c.. |
|||
Particle Size | 4.0 - 7.0 µm | 4.0 - 7.0 µm | d50 |
Magyar Aluminum ALO-DN-4F Alumina Ground Alumina |
|||
Particle Size | 4.0 µm | 4.0 µm | d50 |
Magyar Aluminum ALOLT 704 Aluminum Hydroxide Viscosity Optimized Type |
|||
Particle Size | 4.0 - 8.0 µm | 4.0 - 8.0 µm | d50 |
Magyar Aluminum ALO-P90-06 Alumina Alumina for Polishing |
|||
Particle Size | 4.0 µm | 4.0 µm | Main Break; Fineness of Grind |
Gwent Electronic Materials C2000107P3 Silver Ink Silver Ink C2000107P3 is designed as a termination for single layer PZT ceramics. After firing the film has good adhesion and solderability.The ink is in a ready to use form at a viscosity suitable.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | Main Break; Fineness of Grind |
Gwent Electronic Materials C2010829D2 Silver Ink Silver Ink C2010829D2 is a high definition silver ink for LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the market.The ink has be.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | 3rd Streak; Fineness of Grind |
Gwent Electronic Materials C2021031D2 Electrode Ink Electrode Ink C2021031D2 is a Silver Palladium (85/15) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | 3rd Streak; Fineness of Grind |
Gwent Electronic Materials C2021031D3 Electrode Ink Electrode Ink C2021031D3 is a Silver Palladium (90/10) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | 90% less than |
H.C. Starck Grade B Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Particle Size | 4.0 - 5.0 µm | 4.0 - 5.0 µm | Medium Grain (d50) |
CeramTec Alunit® HS Aluminum Nitride Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I.. |
|||
Particle Size | 4.0 µm | 4.0 µm | D50 (Malvern) Size E |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 4.0 µm | 4.0 µm | D50 (Malvern) Size E |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 4.0 - 7.0 µm | 4.0 - 7.0 µm | Grain Size; Intercept Method |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
Particle Size | 4.0 µm | 4.0 µm | Median |
Excalibar ExBar™ W 4 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Size | 4.0 µm | 4.0 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC12 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 4.0 µm | 4.0 µm | |
China Tungsten YG15 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 4.0 - 6.0 µm | 4.0 - 6.0 µm | Mean particle size |
Carborundum CarboTherm™ CTUF Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |