Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 30 µm | <= 30 µm | 90% smaller than |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | <= 30 µm | <= 30 µm | 90% smaller than |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | 30 µm | 30 µm | median; Microtrac |
Nyco NYGLOS® 20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 30 - 60 µm | 30 - 60 µm | mesh. |
Oceanchem Group Calcium Chloride 94-95% powder Molecular Formula: CaCl2Information Provided by Oceanchem Group |
|||
Particle Size | 30 - 50 µm | 30 - 50 µm | Mean |
Potters Industries Spheriglass® 3000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Size | 30 µm | 30 µm | Geon® DFT 1466; Internal Method |
PolyOne Geon™ FIT E 50 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 50 is a low molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and reduce.. |
|||
Particle Size | 30 - 70 µm | 30 - 70 µm | d50 |
Magyar Aluminum ALO-P54 Alumina Alumina for Polishing |
|||
Particle Size | >= 30 µm | >= 30 µm | 0.3% finer than |
Imerys Minsparâ„¢ 1 Feldspar Minspar 1 is a minus 30 mesh Feldspar product used in the glass container and ceramic tile markets.Information provided by Imerys |
|||
Particle Size | 30 - 38 µm | 30 - 38 µm | 50% |
H.C. Starck Amperit® 519.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Particle Size | 30 - 37 µm | 30 - 37 µm | 90% |
H.C. Starck Amperit® 544.059 Dense Coated Tungsten Carbide-Nickel 83-17 (WC-Ni) |
|||
Particle Size | 30 - 38 µm | 30 - 38 µm | 50% |
H.C. Starck Amperit® 586.1 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Particle Size | 30 - 46 µm | 30 - 46 µm | |
Lucite International Colacryl ® B866 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based homopolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.. |
|||
Particle Size | 30 - 37 µm | 30 - 37 µm | |
H.C. Starck Amperit® 140.3 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | 30 - 37 µm | 30 - 37 µm | |
H.C. Starck Amperit® 146.3 Chromium (Cr) HS Number: 81122031 |
|||
Particle Size | 30 µm | 30 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 607 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 30 µm | 30 µm | |
Silberline Extra Sparkle Silvex® 400-10-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Particle Size | 30 µm | 30 µm | |
Shin-Etsu Silicones KSP-102 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 30 µm | 30 µm | |
Silberline Sparkle Silver® 3666 Sparkle Silver® 3666 is a coarse, bright, regular purity, non-leafing aluminum pigment popular for solvent-based general industrial coatings. This pigment can be used with tints to produce a wide.. |
|||
Particle Size | 30 µm | 30 µm | 99.5% less than value (Size D) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | <= 30 µm | <= 30 µm | |
Epoxy Technology EPO-TEK® OG159-2 UV Cure Optical Epoxy Material Description: A single component, high viscosity, UV curable epoxy adhesive designed for sealing glass plates together in the LCD/OLED/display industry. It contains 1mil glass beads for bon.. |
|||
Particle Size | 30 µm | 30 µm | @ 98% |
CIMBAR Body Filler Talc for Polyester Filler Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes.. |
|||
Particle Size | 30 µm | 30 µm | @ 98%; Micrometrics Sedigraph 5100 |
CIMBAR RP 9310 Talc RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R.. |
|||
Particle Size | 30 µm | 30 µm | 10th% |
3M A16/500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 30 µm | 30 µm | 50th% |
3M H50/10000EPX Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 30 µm | 30 µm | 10th% |
3M K1 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 30 µm | 30 µm | 10th% |
3M K20 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 30 µm | 30 µm | diameter |
3M XLD3000 Glass Bubbles 3M™ Glass Bubbles XLD3000 are high-strength additives for polymers made from a water-resistant and chemically stable soda-lime-borosilicate glass. These hollow glass bubbles can be compounded with .. |
|||
Particle Size | 30 µm | 30 µm | |
3M Dyneon™ PFA 6503PAZ Fluoroplastic Powder 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PAZ is a fluorothermoplastic powder designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tan.. |
|||
Particle Size | 30 µm | 30 µm | |
3M Dyneon™ PFA 6503PBZ Fluoroplastic Powder 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PBZ is a fluorothermoplastic powder with excellent thermal stability characteristics, designed for use in thin film powder coatings. Typical applications i.. |
|||
Particle Size | 30 - 38 µm | 30 - 38 µm | 50% |
H.C. Starck Amperit® 551.074 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni) |