Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 170 - 230 µm | 170 - 230 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9622 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Particle Size | 170 - 265 µm | 170 - 265 µm | |
Lucite International Elvacite ® 2016 Acrylic Resin Elvacite® 2016 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. Elvacite® 2016 is useful in clear, translucent or pigmented metal lacquers. It is a fast dissolvi.. |
|||
Particle Size | 170 - 265 µm | 170 - 265 µm | |
Lucite International Elvacite ® 2697 Acrylic Resin Elvacite® 2697 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. Elvacite® 2697 is useful in clear, translucent or pigmented metal lacquers. It is a fast dissolvi.. |
|||
Particle Size | 170 µm | 170 µm | Before Conversion |
Silberline Silvet® 430-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Particle Size | 170 µm | 170 µm | Before Conversion |
Silberline Silvet® 430-30-E1 Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final processi.. |
|||
Particle Size | 170 µm | 170 µm | |
Silberline Silvex® 430-15-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 170 µm | 170 µm | |
Silberline Silvex® 430-15-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 170 µm | 170 µm | Average; Dp50; ASTM D1921 |
Braskem Idealis 500 High Molecular Weight Polyethylene Powder Braskem Idealis 500 is the only High Molecular Weight Polyethylene resin in powder form specially designed for the compression molding process; Applications range from food handling cutting boards a.. |
|||
Particle Size | 170 µm | 170 µm | Average, Dp50; ASTM-D1921 |
Braskem Idealis 500 Compression Molding High Molecular Weight Polyethylene Braskem Idealis 500 is the only high molecular weight polyethylene resin in powder form specially designed for the compression molding process. Its applications range from food handling, cutting boa.. |