Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 17 µm | 17 µm | median; Microtrac |
Nyco M15 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 17 µm | 17 µm | Median Diameter |
Omya PULPROWHITE® 17 - SA Calcium Carbonate A dry ground calcium carbonate with a broad particle distribution and closely controlled top size.Information supplied by Omya North America. |
|||
Particle Size | 17 - 21 µm | 17 - 21 µm | 10% |
H.C. Starck Amperit® 110.2 Agglomerated Sintered (Mo-Mo2C) |
|||
Particle Size | 17 - 22 µm | 17 - 22 µm | 10% |
H.C. Starck Amperit® 526.062 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 17 - 21 µm | 17 - 21 µm | 10% |
H.C. Starck Amperit® 527.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 17 - 22 µm | 17 - 22 µm | 10% |
H.C. Starck Amperit® 554.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 17 - 21 µm | 17 - 21 µm | 10% |
H.C. Starck Amperit® 588.074 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 45/15 µm |
|||
Particle Size | 17 - 21 µm | 17 - 21 µm | 10% |
H.C. Starck Amperit® 827.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 17 - 22 µm | 17 - 22 µm | 10% |
H.C. Starck Amperit® 832.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 17 - 21 µm | 17 - 21 µm | 10% |
H.C. Starck Amperit® 599.074 Agglomerated Sintered Molybdenum Carbide (Cr2O3) |
|||
Particle Size | 17 µm | 17 µm | Before Conversion |
Silberline Aquavet® 190nl-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline Aquavet® 205-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline EternaBrite® Premier 251 EternaBrite® Premier 251 is a fine, very bright, leafing aluminum pigment with excellent opacity and distinctness of image (D.O.I) for solvent based general industrial coatings. This grade is not.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline EternaBrite® Premier 251-DL EternaBrite® Premier "DL" pigments are leafing aluminum pigment pastes carried in a glycol. These grades are based on cornflake geometry and offer enhanced leafing properties flexographic and gra.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline EternaBrite® Premier 251-PA EternaBrite® Premier pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced leafing properties in solven.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline SparkleBriteâ„¢ 190NL-DL SparkleBriteâ„¢ "DL" pigments are non-leafing aluminum pigment pastes carried in a glycol. These grades are based on cornflake geometry and produce strong metallic effects in flexographic and gra.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline SparkleBriteâ„¢ 190NL-PA SparkleBriteâ„¢ pigments are non-leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and produce strong metallic effects in solvent and wate.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline Sparkle Silver Ultraâ„¢ 6555 Sparkle Silver Ultraâ„¢ grades are very bright lenticular automotive aluminum pigments. They offer a very smooth patina and narrow particle size distribution, allowing the formulator to create ve.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline SparkleBriteâ„¢ Premier 2052NL-DL SparkleBriteâ„¢ Premier "DL" pigments are non-leafing aluminum pigment pastes carried in a glycol. These grades are based on cornflake geometry and produce strong metallic effects in flexographic.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline SparkleBriteâ„¢ Premier 2052NL-PA SparkleBriteâ„¢ Premier pigments are non-leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced metallic effects in s.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline Stamford "O" Standard Series Stamford O is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This is an economical grade with cornflake geometry and wide particle size distribution ra.. |
|||
Particle Size | 17 µm | 17 µm | |
Silberline Tufflake® 3120-AR Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Particle Size | 17 µm | 17 µm | d90, Typical |
TIMCAL TIMREX® C-LUB 306 Primary Synthetic Graphite Information provided by TIMCAL |
|||
Particle Size | 17 µm | 17 µm | d90 |
TIMCAL TIMREX® MX15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 17 - 23 µm | 17 - 23 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6 Information provided by Arkema Group |
|||
Particle Size | 17 - 23 µm | 17 - 23 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 3502 D Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Particle Size | 17 µm | 17 µm | Median |
CIMBAR BARIMITE™ G-50 High Purity Barite (BaSO4) Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemi.. |
|||
Particle Size | 17 - 21 µm | 17 - 21 µm | 10% |
H.C. Starck Amperit® 529.074 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo) |
|||
Particle Size | 17 - 22 µm | 17 - 22 µm | 10% |
H.C. Starck Amperit® 547.059 Tungsten Carbide-Nickel 88-12 (WC-Ni) |
|||
Particle Size | 17 - 21 µm | 17 - 21 µm | 10% |
H.C. Starck Amperit® 551.074 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni) |