Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 12 µm | >= 12 µm | 10% smaller than |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Particle Size | 12 µm | 12 µm | median; Microtrac |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 12 µm | 12 µm | median; Microtrac |
Nyco NYGLOS® MSTPO Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 12 µm | 12 µm | Median Grain Diameter |
Nabaltec APYMAG® 30 Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Particle Size | 12 µm | 12 µm | Median Grain Diameter |
Nabaltec APYRAL® 4 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Particle Size | 12 µm | 12 µm | Median Diameter |
Omya CAL® FG-10 AZ Food Grade Calcium Carbonate A food grade ground limestone that, pursuant to FDA written opinion, may be identified as "calcium carbonate" in the ingredient lists of finished foods.Information supplied by Omya North America. |
|||
Particle Size | 12 µm | 12 µm | Median Diameter |
Omya SNOWHITE® 12 - PT Calcium Carbonate A dry ground calcium carbonate with an intermediate and closely sized particle distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 304L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 317L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 410L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 4140/MA Low Alloy Steel Master Alloy Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.Master alloy blended with 2 parts iron to produ.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 90/10 Cu Sn Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals Co212-e Cobalt Alloy Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals Oxygen-Free Electronic Copper Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 17-4 PH Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.Material Notes: Composition above is typical of.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 420 Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 80/20 Ni Cr Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | mean |
Imerys Minsparâ„¢ 3 Ground Feldspar Minsparâ„¢ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minsparâ„¢ 3 an e.. |
|||
Particle Size | 12 - 16 µm | 12 - 16 µm | 10% |
H.C. Starck Amperit® 584.072 Chromium Carbide-Nickel-Chromium 75-25 (Cr3C2-NiCr) |
|||
Particle Size | 12 µm | 12 µm | |
Shin-Etsu Silicones X-52-7073 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 12 µm | 12 µm | |
Silberline A-6209 A-6209 is a standard grade; class "B", medium sized, leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance |
|||
Particle Size | 12 µm | 12 µm | |
Silberline EternaBrite® Premier 351 EternaBrite® Premier 351 is a fine, very bright, lenticular leafing aluminum pigment with excellent opacity and distinctness of image (D.O.I) for solvent based general industrial coatings. This g.. |
|||
Particle Size | 12 µm | 12 µm | |
Silberline EternaBrite® Premier 351-PA EternaBrite® Premier pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced leafing properties in solven.. |
|||
Particle Size | 12 µm | 12 µm | d90, Typical |
TIMCAL TIMREX® LSG10 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | <= 12 µm | <= 12 µm | Max |
CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4) BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan and BariScan Ultra barite meet and exceed the requireme.. |
|||
Particle Size | <= 12 µm | <= 12 µm | Max |
CIMBAR CIMBAR™ UF Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Size | 12 µm | 12 µm | 10th% |
3M iM16K Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 12 µm | 12 µm | Median Diameter |
Omya OMYACARB® 10 - AZ Calcium Carbonate A dry ground calcium carbonate with an intermediate and closely sized particle distribution.Applications: Am ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 316L/MA Master Alloy Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.Master alloy blended with 2 parts iron to produ.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 440C Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |