Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 11.2 µm | 11.2 µm | median |
Esstech V-117-1112 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |