Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.70 µm | 0.70 µm | |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 0.70 µm | 0.70 µm | |
Nabaltec NABALOX® NO 713-40 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 0.70 µm | 0.70 µm | Median Diameter |
Omya COVERCARB® HP Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating. An opacifying product that is designed to reduce coating costs through the replacement of more expensive pigments. This product is .. |
|||
Particle Size | 0.70 µm | 0.70 µm | Median Diameter |
Omya HYDROCARB® 90 Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Particle Size | 0.70 µm | 0.70 µm | Median Diameter |
Omya HYDROCARB® 90 HS Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Particle Size | 0.70 µm | 0.70 µm | Median Diameter |
Omya HYDROCARB® 95 HS Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Particle Size | 0.70 µm | 0.70 µm | Median Diameter |
Omya OMYACARB® UF - FL Calcium Carbonate A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water.. |
|||
Particle Size | 0.70 µm | 0.70 µm | Median Diameter |
Omya OMYACARB® UTF-FL Calcium Carbonate A high purity, ultrafine, wet ground, surface treated natural calcium carbonate available in dry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such a.. |
|||
Particle Size | 0.70 µm | 0.70 µm | Median Diameter |
Omya OMYAFIL® Calcium Carbonate An ultrafine ground calcium carbonate for paper and board filling.Information supplied by Omya North America. |
|||
Particle Size | 0.70 µm | 0.70 µm | Median Diameter |
Omya OMYAFLOW® UF - SY Calcium Carbonate A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Decorative paints.Information supplied by Omya North America. |
|||
Particle Size | 0.70 µm | 0.70 µm | Mean |
Momentive Performance Materials NX1 Boron Nitride (BN) Powder Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a.. |
|||
Particle Size | 0.70 µm | 0.70 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade UF 10 Silicon Carbide, SiC Alpha SiC for sintering and hot-pressing.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for wa.. |
|||
Particle Size | 0.70 - 1.1 µm | 0.70 - 1.1 µm | d10 |
Indium Corp. In2O3 Type B Indium Oxide, Fine Powder Indium Sesquioxide is a yellow colored powder. It is a stable ceramic-like material, insoluble in water and volatizes at 850°C. Indium sesquioxide is a n-type semiconductor and as such is used .. |
|||
Particle Size | 0.70 µm | 0.70 µm | median |
Esstech Esstech DSS™ V-199-4120 Silinated Dental Glass Esstech DSS™ Glass features optimized levels of silane and improved hydrophobicity, properties which may result in improved adhesion & compatibility of the organic / inorganic surfaces in the compo.. |
|||
Particle Size | 0.70 µm | 0.70 µm | median |
Esstech Esstech DSS™ V-258-4107 Silinated Dental Glass Esstech DSS™ Glass features optimized levels of silane and improved hydrophobicity, properties which may result in improved adhesion & compatibility of the organic / inorganic surfaces in the compo.. |
|||
Particle Size | 0.70 µm | 0.70 µm | D50 |
CIMBAR NANO-FLEX® Talc - D for TPO Applications NANO-FLEX® Talc is designed for use in high performance TPO applications that require high brightness and an high balance of stiffness and toughens. NANO-FLEX® Talc is made by a proprietary proces.. |
|||
Particle Size | 0.70 - 0.90 µm | 0.70 - 0.90 µm | |
C.O.I.M. FILCO® 300 Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber Sizing Description: Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in.. |
|||
Particle Size | 0.70 µm | 0.70 µm | median |
Esstech Esstech DSS™ V-117-4107 Silinated Dental Glass Esstech DSS™ Glass features optimized levels of silane and improved hydrophobicity, properties which may result in improved adhesion & compatibility of the organic / inorganic surfaces in the compo.. |