Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers ROVENE® 4021 SBR Latex ROVENE® 4021 is a “self†cross-linking, carboxylated styrene-butadiene emulsion that has a firm hand with outstanding strength properties. This binder is especially suited for various n.. |
|||
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers ROVENE® 4040 SBR Emulsion ROVENE® 4040 is a non-carboxylated styrene-butadiene (SBR) latex emulsion designed for use as a concrete modifier. ROVENE® 4040 is used as a title grout modifier where it enhances adhesion. It.. |
|||
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers ROVENE® 4150 SBR Latex ROVENE® 4150 is a medium-firm, self-XLing, carboxylated styrene-butadiene (SBR) latex emulsion. Its styrene content (55%) permits its use in formulating carpet and flooring mastics. This versatil.. |
|||
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers ROVENE® 4170 SBR Latex ROVENE® 4170 is a carboxylated styrene-butadiene emulsion that has a medium-firm hand with outstanding strength properties. This binder is especially suited for various textile and coating applic.. |
|||
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers ROVENE® 4176 SBR Latex ROVENE® 4176 is a medium-soft carboxylated styrene-butadiene (SBR) latex emulsion. Its styrene content (50%) permits its use in formulating carpet laminating adhesives and flooring mastics. This .. |
|||
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers Rovene® 6018 Styrene-Acrylic Emulsion Applications: Rovene® 6018 is a silanated styrene-acrylic emulsion specifically designed for formulation of construction adhesives such as ceramic tile mastics and carpet adhesives. It provides e.. |
|||
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers ROVENE® 6020 SBR Latex Applications: Rovene® 6020 is a soft, carboxylated stryene-acrylic copolymer emulsion. The typical films are soft and strong with good water resistance and exhibit good resistance to discoloratio.. |
|||
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers Rovene® 6118 Styrene-Acrylic Emulsion Applications: Rovene® 6118 is a silanated styrene-acrylic emulsion specifically designed for formulation of concrete sealers and performance coatings. It provides excellent adhesion to concrete a.. |
|||
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers Rovene® 8001 Hybrid Styrene-Butadiene Emulsion Rovene® 8001 is a hybrid of natural binder and self crosslinking carboxylated styrene-butadiene emulsion developed especially for use on organic spunbond roofing mats where it imparts excellent t.. |
|||
Particle Size | 0.15 - 0.50 µm | 0.15 - 0.50 µm | Dispersed |
Shamrock Technologies NanoFLON® P 47A Thermoplastic Grade PTFE Additive Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro.. |
|||
Particle Size | 0.15 - 0.20 µm | 0.15 - 0.20 µm | Grain; DIN EN 623-3 |
CeramTec MZ 111 Zirconia, ZrO2-Y2O3 MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications. |
|||
Particle Size | 0.15 - 0.35 µm | 0.15 - 0.35 µm | |
Daikin POLYFLON D-2CE PTFE Dispersion POLYFLON PTFE aqueous dispersions are normally stabilized with non-ionic surfactants and contain 60% POLYFLON PTFE by weight.Processing Methods: Impregnation.Applications: Impregnated glass fabric.I.. |
|||
Particle Size | 0.15 - 0.35 µm | 0.15 - 0.35 µm | |
Daikin POLYFLON D-2E PTFE Dispersion POLYFLON PTFE aqueous dispersions are normally stabilized with non-ionic surfactants and contain 60% POLYFLON PTFE by weight.Processing Methods: Impregnation.Applications: Impregnated glass fabric.I.. |
|||
Particle Size | 0.15 - 0.60 µm | 0.15 - 0.60 µm | MA147LFE |
C.O.I.M. FILCO® 306 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Particle Size | 0.15 µm | 0.15 µm | |
Mallard Creek Polymers ROVENE® 4475 SBR Latex ROVENE® 4475 is a carboxylated styrene-butadiene emulsion that has a very firm hand with outstanding strength properties. This binder can accept high filler loads of calcium carbonate, clays, and a.. |