Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | outside diameter |
NanoAmor 90%, OD/ID: 10-30/3-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | outside diameter |
NanoAmor 95% 10-20 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 10-20/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 10-30/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | outside diameter |
NanoAmor 95%, OD/ID: 10-20/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | outside diameter |
NanoAmor 95%, OD: 10-20 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID: 10-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Boron Carbide Nanoparticles General DescriptionBoron Carbide (BC) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Carbide Particles are typically 10 - 100 nanometers (nm) with s.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Boron Nitride Nanoparticles General DescriptionBoron Nitride (BN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Nitride Particles are typically 10 - 100 nanometers (nm) with s.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Erbium Nanoparticles General DescriptionErbium (Er) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Erbium Particles are typically 10 - 80 nanometers (nm) with specific s.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Lanthanum Oxide Nanopowder General DescriptionLanthanum Oxide (LaO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Lanthanum Oxide Particles are typically 10-30 nanomete.. |
|||
Particle Size | 0.010 - 0.050 µm | 0.010 - 0.050 µm | |
American Elements Lithium Manganese Dioxide Nanoparticles General DescriptionLithium Manganese Oxide (LiMnO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Manganese Oxide Particles are typically 10 - 50 na.. |
|||
Particle Size | 0.010 - 0.050 µm | 0.010 - 0.050 µm | |
American Elements Lithium Nanoparticles General DescriptionLithium (Li) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lithium Particles are typically 10 - 50 nanometers (nm) with specific.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Lithium Vanadate Nanoparticles General DescriptionLithium Vanadate or Lithium Vanadium Oxide (LiVO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Vanadate or Lithium Vanadium Oxi.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Lutetium Nanoparticles General DescriptionLutetium (Lu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lutetium Particles are typically 10 - 100 nanometers (nm) with speci.. |
|||
Particle Size | 0.010 - 0.045 µm | 0.010 - 0.045 µm | |
American Elements Neodymium Nanoparticles General DescriptionNeodymium (Nd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Neodymium Particles are typically 10 - 45 nanometers (nm) with spec.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Nickel Oxide Nanopowder General DescriptionNickel Oxide (NiO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Nickel Oxide Particles are typically 10-30 nanometers (nm.. |
|||
Particle Size | 0.010 - 0.040 µm | 0.010 - 0.040 µm | |
American Elements Nickel Titanium Nanoparticles General DescriptionNickel Titanium (NiTi) Nanoparticles, nanodots or nanopowder are black spherical high surface area alloy particles. Nanoscale Nickel Titanium Particles are typically 10 - 40 nanom.. |
|||
Particle Size | 0.010 - 0.050 µm | 0.010 - 0.050 µm | |
American Elements Samarium Nanoparticles General DescriptionSamarium (Sm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Samarium Particles are typically 10 - 50 nanometers (nm) with specif.. |
|||
Particle Size | 0.010 - 0.15 µm | 0.010 - 0.15 µm | |
American Elements Silicon Carbide Nanoparticles General DescriptionSilicon Carbide (SiC) Nanoparticles, whiskers, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Carbide Particles are typically 10 - 150 nanomet.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Silicon Nanotubes General DescriptionSilicon (Si) Nanotubes, Single-Walled, Double Walled and Multi-Walled are tubular ultra high surface area nanotubes. Nanoscale Silicon Nanotubes are typically 10 - 100 nanometers .. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Silicon Nitride Nanoparticles General DescriptionSilicon Nitride (SiN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Nitride Particles are typically 10 - 100 nanometers (nm) w.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | |
American Elements Tantalum Nanoparticles General DescriptionTantalum (Ta) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tantalum Particles are typically 10-20 nanometers (nm) wi.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Terbium Nanoparticles General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific.. |
|||
Particle Size | 0.010 - 0.20 µm | 0.010 - 0.20 µm | |
American Elements Terbium Oxide Nanopowder General DescriptionTB-MITE powders and dispersions are inorganic terbium-oxide nanoparticles. TB-MITE-A products are uncoated and hydrophilic. TB-MITE-O products are coated with an organic silane (1.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | |
American Elements Tin Nanoparticles General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specifi.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Titanium Nitride Nanoparticles General DescriptionTitanium Nitride (TiN) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Titanium Nitride Particles are typically 10 - 100 nanometer.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Vanadium Oxide Nanopowder General DescriptionVanadium Oxide (VO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Vanadium Oxide Particles are typically 10-30 nanometers .. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Calcium Phosphate Nanoparticles General DescriptionCalcium Phosphate (CAP) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Phosphate Particles are typically 10 - 80 nanometers (nm.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Copper Nanoparticles General DescriptionCopper (Cu) Nanoparticles, nanodots or Nanopowder are black brown spherical high surface area metal particles. Nanoscale Copper Particles are typically 10-30 nanometers (nm) with .. |