Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 430 - 600 µm | 430 - 600 µm | |
Potters Industries A-Series P-0230 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 300 - 600 µm | 300 - 600 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres EXTENDOSPHERESâ„¢300/600 are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, they can .. |
|||
Particle Size | 500 - 600 µm | 500 - 600 µm | |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Particle Size | 230 - 600 µm | 230 - 600 µm | Average value: 538 µm Grade Count:6 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |