Polymer Property : Particle Size = 39 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 31 - 39 µm
31 - 39 µm
50%
H.C. Starck Amperit® 588.074 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 45/15 µm
Particle Size 31 - 39 µm
31 - 39 µm
50%
H.C. Starck Amperit® 827.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3)
Particle Size 31 - 39 µm
31 - 39 µm
50%
H.C. Starck Amperit® 529.074 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo)
Particle Size 31 - 39 µm
31 - 39 µm
50%
H.C. Starck Amperit® 584.054 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)