Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 25 - 29 µm | 25 - 29 µm | 90% |
H.C. Starck Amperit® 251 Gas Atomized (NiCr 80-20) |
|||
Particle Size | 25 - 29 µm | 25 - 29 µm | 90% |
H.C. Starck Amperit® 281 Gas Atomized (NiAl 95-5) |