Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 8.9 - 28 µm | 8.9 - 28 µm | d50 |
Indium Corp. In(OH)3 Crystalline Indium Hydroxide Indium Acetate is a white powder. Crystalline Form: Primary particles range from 1 to 5 microns in size. They are cubic in shape and form agglomerates up to approximately 35 microns.PropertiesChe.. |
|||
Particle Size | 18 - 28 µm | 18 - 28 µm | D(0.5) |
Akzo Nobel Expancel® 551 DE 20 d60 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 22 - 28 µm | 22 - 28 µm | 50% |
H.C. Starck Amperit® 552.072 Tungsten Carbide - Chromium Carbide-Nickel 73-20-7 (WC-CrC-Ni) |