Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Granulate Size |
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9216 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9612 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9620 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 170 - 230 µm | 170 - 230 µm | Mean Granulate Size |
Nabaltec GRANALOX® NM 9622 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9622 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9816 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 180 - 230 µm | 180 - 230 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9923 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 110 - 230 µm | 110 - 230 µm | |
Lucite International Elvacite ® 2021 Acrylic Resin Elvacite® 2021 is a high molecular weight methyl methacrylate polymer. It is used in barrier coatings for vinyl. Its high molecular weight provides excellent abrasion resistance.Information provide.. |