Polymer Property : Particle Size = 22 µm
Polymer Property :
Particle Size =
22 µm
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Particle Size
18
-
22
µm
18
-
22
µm
10%
H.C. Starck Amperit® 105.074 Agglomerated Sintered Molybdenum (Mo)
Particle Size
17
-
22
µm
17
-
22
µm
10%
H.C. Starck Amperit® 526.062 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Particle Size
18
-
22
µm
18
-
22
µm
10%
H.C. Starck Amperit® 526.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Particle Size
17
-
22
µm
17
-
22
µm
10%
H.C. Starck Amperit® 554.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size
18
-
22
µm
18
-
22
µm
10% for WC-Co 83-17
H.C. Starck Amperit® 560.062 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60)
Composition is of NiSF RC 60 only
Particle Size
17
-
22
µm
17
-
22
µm
10%
H.C. Starck Amperit® 832.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3)
Particle Size
18
-
22
µm
18
-
22
µm
Average; ATO 40-41-0 (Coulter Counter)
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved
Information provided by Arkema Group
Particle Size
17
-
22
µm
17
-
22
µm
10%
H.C. Starck Amperit® 547.059 Tungsten Carbide-Nickel 88-12 (WC-Ni)