Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 15 - 17 µm | 15 - 17 µm | 50% |
H.C. Starck Amperit® 553.065 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 8.0 - 17 µm | 8.0 - 17 µm | For Median |
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder CIMBAR's Crescent product line is a natural calcium carbonate ground to various particle size distributions. The crystalline structure of the calcium carbonate in Crescent products has a predominan.. |
|||
Particle Size | 10 - 17 µm | 10 - 17 µm | D(0.5) |
Akzo Nobel Expancel® 092 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |