Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 45 - 151 µm | 45 - 151 µm | Range (D10 to D90); Laser Diffraction |
ALM D80-ST Nylon 11 SLS Prototyping Polymer Unfilled, color stabilized nylon 11 material that is also stabilized to prevent premature thermal degradation. Parts produced from PA D80-ST exhibit superior mechanical properties. Relatively inexp.. |
|||
Particle Size | 45 - 151 µm | 45 - 151 µm | Range (D10 to D90); Laser Diffraction |
ALM FR 106 Nylon 11 SLS Prototyping Polymer This flame retardant rapid prototyping material has additives in the raw material that allows it to pass aeronautic standard FAR25.853 smoke, flame, and toxicity tests. This material is ideal for Ae.. |