Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.15 - 0.35 µm | 0.15 - 0.35 µm | |
Daikin POLYFLON D-2CE PTFE Dispersion POLYFLON PTFE aqueous dispersions are normally stabilized with non-ionic surfactants and contain 60% POLYFLON PTFE by weight.Processing Methods: Impregnation.Applications: Impregnated glass fabric.I.. |
|||
Particle Size | 0.15 - 0.35 µm | 0.15 - 0.35 µm | |
Daikin POLYFLON D-2E PTFE Dispersion POLYFLON PTFE aqueous dispersions are normally stabilized with non-ionic surfactants and contain 60% POLYFLON PTFE by weight.Processing Methods: Impregnation.Applications: Impregnated glass fabric.I.. |
|||
Particle Size | 0.25 - 0.35 µm | 0.25 - 0.35 µm | Grain |
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade ATZ is an alumina toughened zirconia used in dental applications. |