Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.050 - 0.080 µm | 0.050 - 0.080 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 50-80/5-15 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.050 - 0.080 µm | 0.050 - 0.080 µm | outside diameter |
NanoAmor 95%, OD: 50-80 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.050 - 0.080 µm | 0.050 - 0.080 µm | outside diameter |
NanoAmor 95%, OD: 50-80 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.050 - 0.080 µm | 0.050 - 0.080 µm | outside diameter |
NanoAmor 95%, OD/ID: 50-80/5-15 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Antimony Oxide Nanopowder General DescriptionAntimony Oxide ( SbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Bismuth Oxide Nanopowder General DescriptionBismuth Oxide ( BiO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Calcium Carbonate Nanoparticles General DescriptionCalcium Carbonate (CaCO3) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Carbonate Particles are typically 10 - 80 nanometers (.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Dysprosium Nanoparticles General DescriptionDysprosium (Dy) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 10 - 80 nanometers (nm) with sp.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Dysprosium Oxide Nanopowder General DescriptionDysprosium (DyO) Oxide Nanopowder or Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Oxide Particles are typically 10 -.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Erbium Nanoparticles General DescriptionErbium (Er) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Erbium Particles are typically 10 - 80 nanometers (nm) with specific s.. |
|||
Particle Size | 0.030 - 0.080 µm | 0.030 - 0.080 µm | |
American Elements Holmium Nanoparticles General DescriptionHolmium (Ho) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 30 - 80 nanometers (nm) with speci.. |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Molybdenum Oxide Nanopowder General DescriptionMolybdenum Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles... |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Tantalum Oxide Nanopowder General DescriptionTantalum Oxide ( TaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Terbium Nanoparticles General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Titanium Nanoparticles General DescriptionTitanium (Ti) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Titanium Particles are typically 10 - 80 nanometers (nm) .. |
|||
Particle Size | 0.040 - 0.080 µm | 0.040 - 0.080 µm | |
American Elements Tungsten Nanoparticles General DescriptionTungsten (W) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Tungsten Particles are typically 40-80 nanometers (nm) with spe.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Ytterbium Nanoparticles General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec.. |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Calcium Oxide Nanopowder General DescriptionCalcium Oxide ( CaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Calcium Phosphate Nanoparticles General DescriptionCalcium Phosphate (CAP) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Phosphate Particles are typically 10 - 80 nanometers (nm.. |