Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 90 µm | 90 µm | Finer than |
Inhance Fluoro-Seal INHANCE® UH-1500 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Particle Size | 90 µm | 90 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 105.2 Agglomerated Sintered Molybdenum (Mo) |
|||
Particle Size | 90 µm | 90 µm | Maximum of 5% greater than, (Mo) |
H.C. Starck Amperit® 119.075 Molybdenum-Nickel SF RC 60 75-25 (Mo / NiSF) Composition is of NiSF RC 60 only |
|||
Particle Size | 90 µm | 90 µm | Maximum of 7% greater than |
H.C. Starck Amperit® 175.2 Nickel (Ni) |
|||
Particle Size | <= 90 µm | <= 90 µm | Maximum of 10% greater than |
H.C. Starck Amperit® 205.5 Dense Coated Nickel Graphite 75-25 (Ni-C) |
|||
Particle Size | 90 µm | 90 µm | Maximum of 7% greater than |
H.C. Starck Amperit® 251.2 Gas Atomized (NiCr 80-20) |
|||
Particle Size | 90 µm | 90 µm | Maximum of 7% greater than |
H.C. Starck Amperit® 280.2 Water Atomized (NiAl 95-5) |
|||
Particle Size | 90 µm | 90 µm | Maximum of 7% greater than |
H.C. Starck Amperit® 281.2 Gas Atomized (NiAl 95-5) |
|||
Particle Size | 90 µm | 90 µm | Maximum of 7% greater than |
H.C. Starck Amperit® 415.2 CoNiCrAlY (MCrAlY) |
|||
Particle Size | 90 µm | 90 µm | Minimum of 98% less than |
H.C. Starck Amperit® 515.2 Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12 HS Number: 28499030 |
|||
Particle Size | 90 µm | 90 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 518.002 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Particle Size | 90 µm | 90 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 583.2 Chromium Carbide-Nickel 83-17 (Cr3C2-Ni) |
|||
Particle Size | 90 µm | 90 µm | Minimum of 95% less than |
H.C. Starck Amperit® 782.2 Titanium Oxide (TiO2) |
|||
Particle Size | <= 90 µm | <= 90 µm | |
H.C. Starck Baymetec® Tungsten Silicide, WSi2 Baymetec® Silicides are highly purity powders manufactured for exacting semiconductor and electronic applications.Low holmic gate electrodes in FET`sInterconnects in VLSIMetallization of compound.. |
|||
Particle Size | 90 µm | 90 µm | Minimum of 95% less than |
H.C. Starck Amperit® 740.2 Aluminum Oxide (Al2O3) |
|||
Particle Size | 90 µm | 90 µm | <0.5 g/kg greater than value; ISO 1624 |
SolVin 266SF Polyvinyl Chloride Pastes - filler Polymers Made by suspension polymerisation.
APPLICATIONS
Filler polymer for plastisols
- Floor covering : hard-wearing top coats, chemically blown and mechanical foams, impregnation layers
- Wall coverings
-.. |
|||
Particle Size | 90 µm | 90 µm | <1 g/kg greater than value; ISO 1624 |
SolVin 561SF Vinyl Chloride - Vinyl Acetate copolymer Paste - filler Made by suspension polymerization.
APPLICATIONS
This resin has been especially developed for automotive mastics.Information provided by SolVin. |
|||
Particle Size | 90 - 100 µm | 90 - 100 µm | 150 mesh; PS-1-2 |
Solvay JAGUAR® HP 105 Surfactant Description: Clear grade with excellent wet combing and detangling benefits. Recommended for use in a broad range of conditioning shampoos.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: H.. |
|||
Particle Size | >= 90 µm | >= 90 µm | 150 Mesh; RP-0887 |
Solvay JAGUAR® HP 120 Surfactant Description: Best suited for use with solvents, even 100% ethanol based formulations. Jaguar HP 120 is a natural thickener and film former for hand sanitizersChemical Name: HYDROXYPROPYL GUARC.T.F.A.. |
|||
Particle Size | >= 90 µm | >= 90 µm | 150 Mesh; RP-0887 |
Solvay JAGUAR® HP 8 COS Surfactant Description: Hydroxypropyl Guar for thickening, which provides a fluid and smooth wet feel to formulationsChemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: Hydroxypropyl GuarCAS: 39421-75-5S.. |
|||
Particle Size | >= 90 µm | >= 90 µm | 150 Mesh; PS-1-2 |
Solvay JAGUAR® HP 8FF Surfactant Description: Hydroxypropyl guar with extremely low residue, designed to be easily dispersed into water where it will wet out and hydrate, forming a viscous HPG fluid which will readily crosslink wit.. |
|||
Particle Size | >= 90 µm | >= 90 µm | thru 150 Mesh; RP-0887 |
Solvay JAGUAR® C 17 Surfactant Description: Highly substantive to hair and skin. Recommended for high conditioning shampoos and moisturizing body washes. Enhances deposition of actives such as silicone, anti-dandruff agents and m.. |
|||
Particle Size | 90 µm | 90 µm | 90th% |
3M A20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 90 µm | 90 µm | 90th% |
3M H20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 90 µm | 90 µm | 90th% |
3M K20 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 90 µm | 90 µm | 90th% |
3M K25 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 90 µm | 90 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 415.079 CoNiCrAlY (MCrAlY) |
|||
Particle Size | 90 µm | 90 µm | Minimum of 95% less than |
H.C. Starck Amperit® 570.2 Sintered Titanium Carbide (TiC) |
|||
Particle Size | 90 µm | 90 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 525.2 Sintered Tungsten Carbide - Cobalt (WC-Co) 83-17 HS Number: 28499030 |
|||
Particle Size | 90 µm | 90 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 547.002 Tungsten Carbide-Nickel 88-12 (WC-Ni) |