Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 9.0 µm | <= 9.0 µm | 90% smaller than |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Particle Size | 9.0 µm | 9.0 µm | median; Microtrac |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | <= 9.0 µm | <= 9.0 µm | Average; Internal Method |
Solvay Specialty Polymers Algoflon® L206 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L206 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It is specially recommended for use as an additive in elastomers (e.g. perfluoroelastomers) t.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 750 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 9.0 - 11 µm | 9.0 - 11 µm | Average |
Malvern Minerals Trikup® PM Silane Treated Aluminum Hydroxide Trikup® is a custom, silane treated alumina trihydrate or aluminum hydroxide. ATH is the largest volume flame retardant in the world. Trikup® adds additional functionality through the use of .. |
|||
Particle Size | 9.0 µm | 9.0 µm | 90% |
Minelco UltraCarb LH15 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 90% |
Minelco UltraCarb LH15C-10 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 90% |
Minelco UltraCarb LH15X Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 9.0 µm | 9.0 µm | Mean |
Momentive Performance Materials AC6069 Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powder grade AC6069 consists of single-crystal hexagonal particles with an average particle size of 9 µm. AC6069 has a relatively tight particle size distr.. |
|||
Particle Size | 9.0 µm | 9.0 µm | Mean |
Momentive Performance Materials NX9 Boron Nitride (BN) Powder Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 50% of particles, (TF Powder) |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 9.0 µm | 9.0 µm | |
Silberline Extra Fine "P" Extra Fine "P" is a standard polished grade; class "A", fine, leafing aluminum pigment carried in mineral spirits.Applications: Trade & Maintenance |
|||
Particle Size | 9.0 µm | 9.0 µm | |
Silberline L-2422-PA L-2422PA is a small particle size, bright leafing aluminum pigment based on standard cornflake geometry. It is a cost effective pigment for producing strong metallic effects with good coverage in li.. |
|||
Particle Size | 9.0 µm | 9.0 µm | Before Conversion |
Silberline Silvet® 220-20-E Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatible with.. |
|||
Particle Size | 9.0 µm | 9.0 µm | |
Silberline "A" Series A-1592FG A-1592FG is a very fine, high opacity, non-leafing aluminum pigment for solvent based industrial coatings. Due to the small particle size, this grade is well suited for imparting high opacity at low.. |
|||
Particle Size | 9.0 - 15.5 µm | 9.0 - 15.5 µm | d90, Guaranteed |
TIMCAL TIMREX® SFG10 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 9.0 µm | 9.0 µm | Median |
CIMBAR EliteTalc® 21 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |
|||
Particle Size | 9.0 µm | 9.0 µm | D50 |
CIMBAR RP 9410 Talc RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are.. |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | D(0.5) |
Akzo Nobel Expancel® 461 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 9.0 µm | 9.0 µm | 90" Percentile |
3M W-210 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Particle Size | <= 9.0 µm | <= 9.0 µm | average |
Oceanchem Group Magnesium Hydroxide Molecular Formula: Mg(OH)2Cas No.: 1309-42-8Use: Magnesium hydroxide is a non-halogen flame retardant recommended where use of halogenated products is limited or prohibited. In addition, it is an e.. |
|||
Particle Size | 9.0 - 13 µm | 9.0 - 13 µm | 10% |
H.C. Starck Amperit® 529.053 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo) |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | D(0.5) |
Akzo Nobel Expancel® 051 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |