Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 85 µm | 85 µm | Mean |
Potters Industries Q-Cel® 7023S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | <= 85 µm | <= 85 µm | d50 |
Magyar Aluminum ALO-B15 Alumina Calcined Alumina; Minimum 5% alpha-Al2O3. |
|||
Particle Size | 85 - 99 µm | 85 - 99 µm | 90% |
H.C. Starck Amperit® 827.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 85 - 99 µm | 85 - 99 µm | 90% |
H.C. Starck Amperit® 832.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | >= 85 µm | >= 85 µm | 200 Mesh; PS-1-1 |
Solvay JAGUAR® S Surfactant Description: 100% Natural thickening polymer. Approved by Ecocert.Chemical Name: Guar Gum C.T.F.A./I.N.C.I. Name: Cyamopsis Tetragonoloba (Guar) Gum CAS: 9000-30-0 Ingredient Compatibility: Anionic,.. |
|||
Particle Size | 85 µm | 85 µm | d90 |
TIMCAL TIMREX® BNB90 Expanded Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | <= 85 µm | <= 85 µm | Max |
CIMBAR BARIMITE™ 200 High Purity Barite (BaSO4) Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemi.. |
|||
Particle Size | 85 µm | 85 µm | D50 |
ALM TPE-210-S Prototyping Polymer A thermoplastic elastomer used to produce parts with “rubber like” qualities. TPE 210-S exhibits good feature definition and infiltration with polyurethane will impart even higher toughness and ab.. |
|||
Particle Size | 85 µm | 85 µm | Effective Top Size |
3M K37 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 85 µm | 85 µm | Effective Top Size |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 85 µm | 85 µm | Effective Top Size |
3M S38HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 85 µm | 85 µm | mean value |
Potters Industries Q-Cel® 6014 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |