Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 75 µm | <= 75 µm | |
Ferro EG 2018 Display Device Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and .. |
|||
Particle Size | <= 75 µm | <= 75 µm | REG Powder |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | <= 75 µm | <= 75 µm | d50 |
Magyar Aluminum ALO-Ex34 Alumina Calcined Alumina |
|||
Particle Size | <= 75 µm | <= 75 µm | d50 |
Magyar Aluminum ALO-ExGB1 Alumina Calcined Alumina |
|||
Particle Size | 75 - 95 µm | 75 - 95 µm | Laser Light Scattering Method; LSY-QB-ID016 |
LG Chemical Lutex 704 SBR Latex Description: Binding Force, Print gloss, High Shear Rheology, Coater RunnabilityApplication: Art Paper-Single, Pre-Film, Blade Coater, Adhesive coated paper and Carpet back-coating adhesiveCSA No. 7.. |
|||
Particle Size | 75 µm | 75 µm | Maximum of 2% greater than |
H.C. Starck Amperit® 821.084 Zirconia-Yttria 80-20 (ZrO2-Y2O3) |
|||
Particle Size | 75 - 105 µm | 75 - 105 µm | |
Lucite International Lucite® 6751 Acrylic Bead Resin Lucite® acrylic resins are used in a variety of industrial, commercial and architectural applications. They’re a favorite among manufacturers of commemorative embedments because of their exc.. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro CF 1417 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific ther.. |
|||
Particle Size | <= 75 µm | <= 75 µm | VEG Powder |
Ferro EG 2928 Glaze and Sealant Glass Glass Type: Pb-Zn-B Typical Powder Form: VEG, MVG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective an.. |
|||
Particle Size | <= 75 µm | <= 75 µm | REG Powder |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 75 µm | 75 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 335.063 Nickel Self-fluxing Alloy HRC 60 (NiCrBSi) |
|||
Particle Size | <= 75 µm | <= 75 µm | 100 |
Solvay Chemicals Ixper® 60C Calcium Peroxide IXPER® 60C is a Calcium Peroxide powder used in a wide range of applications in environmental, seed coating, baking e.g. marketsEINECS Number: 215-139-4/CAS Number: 1305-79-9Information provided .. |
|||
Particle Size | <= 75 µm | <= 75 µm | Scattered Fineness |
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder Conformable with: Q/DYS 014-2007Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resist.. |
|||
Particle Size | <= 75 µm | <= 75 µm | <5%; TI-2087 |
Solvay RHODOPOL® G Surfactant Description: Rhodopol® G is granular and dust free grade of Xanthan Gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent. It has rapid hydration propertie.. |
|||
Particle Size | 75 µm | 75 µm | at a density of 1.73 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | Springback 17%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | Springback 17%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS5-44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | Springback 17%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS5-75TT Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | at a density of 2.03 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | springback 23%, pressure of 0.477 t/cc |
TIMCAL TIMREX® T44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | Springback 6.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | <= 75 µm | <= 75 µm | < 3.0 wt% above |
Excalibar NewBar™ API Barite BaSO4 Powder NewBar™ API barite product is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas explorati.. |
|||
Particle Size | 75 µm | 75 µm | 90th% |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 75 µm | 75 µm | Effective Top Size |
3M S22 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro CF 7570 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific ther.. |
|||
Particle Size | 75 µm | 75 µm | 92 min, 200 mesh; TI-2087 |
Solvay RHODICARE H Surfactant Description: Rhodicare® H is an anionic bio-polymer with excellent stabilizing, thickening and suspending properties. It has high electrolyte stability over a wide range of pH and fast hydration ra.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro CF 7572 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci.. |
|||
Particle Size | <= 75 µm | <= 75 µm | VSD Powder |
Ferro CF 7575 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci.. |