Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 304L Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 304L/MA Master Alloy Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.Master alloy blended with 2 parts iron to pr.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 310S Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 316L Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 316L/MA Master Alloy Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.Master alloy blended with 2 parts iron to pr.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 317L Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 410L Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80 % < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 4140/MA Low Alloy Steel Master Alloy Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.Master alloy blended with 2 parts iron to pr.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 420/MA Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.Master alloy blended with 3 parts iron to pr.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 430L Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80 % < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 440C Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80 % < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 49FeCo2V Cobalt Alloy Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 80/20 Ni Cr Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 90/10 Cu Sn Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals Co452 Cobalt Alloy Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals Fe30Cr Binary Alloy Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals Fe3Si Binary Alloy Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals Fe50Cr Binary Alloy Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals M2 Tool Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals M2/MA Tool Steel Master Alloy Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.Master alloy blended with 2 parts iron to pr.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals Ni40Cu Binary Alloy Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals Oxygen-Free Electronic Copper Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals S2 Tool Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 17-7 PH Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 420 Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80 % < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals Co552 Cobalt Alloy Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals Cu10Al Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals D2 Tool Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 17-4 PH Stainless Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.Material Notes: Composition above is typical.. |
|||
Particle Size | 6.7 µm | 6.7 µm | Mean |
Osprey Metals 4365 Low Alloy Steel Powder (Grade 95% - 16) Particle size distribution 1-250 microns. Typical distribution:98% < 22 microns95% < 16 microns80% < 10 microns26% < 5 micronsMean size is 6.7 microns.SHAPE: Predominantly spherical PACKAGING: .. |