Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 500 - 710 µm | 500 - 710 µm | |
Potters Industries A-Series P-0280 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 500 µm | 500 µm | ASTM D4895 |
3M Dyneon™ TFM™ 2001 Modified PTFE Paste Extrusion Powder
(discontinued **) Type I, gr. 2 PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1000. Average particle size 500µm.Modified PTFE fine powder product for paste extrusion applications. The modified .. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TF 2021 PTFE
(discontinued **) Processable by standard paste extrusion methodsBoth grades can be processed at low to medium reduction ratiosTF 2021 PTFE is preferred for unsintered thread sealing tapes and expanded joint sealants.. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TFM™ 2001 PTFE
(discontinued **) Processable by standard paste extrusion methodRecommended for high performance applications with reduction ratios up to 1000:1Provides denser polymer structure with fewer micro voids and lower gas p.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5053 500 Micron LDPE Powder Description: ICOFLO 510-5053 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5073 500 Micron LLDPE Powder Description: ICOFLO 510-5073 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5059 500 Micron LDPE Powder Description: ICOTEX 520-5059 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Information provided by ICO Polymers.A Sch.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5062 500 Micron LDPE Powder Description: ICOTEX 520-5062 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, .. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5076 500 Micron EVA Powder Description: ICOTEX 520-5076 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Its key characteristics are a good melt flow and flexibility,.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 160 SP Dry Air-Setting Refractory Mortar Description: Adhesiet 160 SP is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the addition of phosphate this material is very good resistant against slag attack.Remarks.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 170 P Al Dry Air-Setting Refractory Mortar Description: Adhesiet 170 P Al is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the special choice of raw materials this mortar is especially applied in aluminum meltin.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET A Dry Air-Setting Refractory Mortar Description: Adhesiet A is a general purpose air setting mortar, supplied as a dry powder for use up to 1400°C.Remarks: Adhesiet mortars can be stored for an unlimited time if kept dry and cool. .. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET B Dry Air-Setting Refractory Mortar Description: Adhesiet B is a general purpose air setting mortar, supplied as a dry powder for use up to 1300°C.Remarks: Adhesiet mortars can be stored for an unlimited time if kept dry and cool. .. |
|||
Particle Size | <= 500 µm | <= 500 µm | ASTM D1921 |
Micropol HD Polyethylene powders for cleaning products Information provided by Micropol Limited |
|||
Particle Size | 500 - 900 µm | 500 - 900 µm | |
Shandong Dongyue Polymer DF-21A PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Particle Size | <= 500 µm | <= 500 µm | |
Shandong Dongyue Polymer DF-21B PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Particle Size | 500 µm | 500 µm | |
Sterigenics Raprex® R-400C Thermoplastic Powder Applications: Extrusion CoatingsA thermoplastic powder based on polyethylene was developed by Sterigenics Advanced Applications for extrusion coating on metal and other surfaces. RAPREX™ 400 is.. |
|||
Particle Size | 500 - 1000 µm | 500 - 1000 µm | 50% Min; 540MA3C5E |
Solvay MIRAPOL® SURF-S 410 Surfactant Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â.. |
|||
Particle Size | 500 - 2000 µm | 500 - 2000 µm | >90 |
Solvay Chemicals Ixper® 70C Calcium Peroxide IXPER® 70C Calcium Peroxide Granules are based on our commercial grade IXPER® 75C.EINECS Number: 215-139-4/CAS Number: 1305-79-9Information provided by Solvay |
|||
Particle Size | >= 500 µm | >= 500 µm | d90, 22%, Vibrated sieving |
TIMCAL TIMREX® KS150-600SP Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 500 µm | 500 µm | |
Daikin POLYFLON F-201 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Particle Size | 500 µm | 500 µm | |
Daikin POLYFLON F-302 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by .. |
|||
Particle Size | 500 - 600 µm | 500 - 600 µm | |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Particle Size | 500 µm | 500 µm | |
Asahi Glass Fluon® CD090 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 13320 |
3M Dyneon™ TF 2025Z PTFE Fine Powder Dyneon™ TF 2025 Z PTFE is an ideal grade for pipe liner applications in chemical plant construction due to high green strength.Product Features:High molecular weightFine powder grade for low to med.. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TF 2029Z PTFE Fine Powder Dyneon™ TF 2029 Z PTFE is an ideal grade for tapes with high mechanical strength, such as electrical tape for wrapped insulations or flat cables. Also ideal for yarn applications, including sewing .. |
|||
Particle Size | 500 µm | 500 µm | VW-10200RP; D90 Particle sizes by sieve measurement |
Solvay Specialty Polymers Virantage® VW-10200 RP, RFP, RSFP Polyethersulfone (PESU)
(Unverified Data**)&l Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial propertie.. |