Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 50.0 - 75.0 µm | 50.0 - 75.0 µm | D 0.5, SATP-114, Malvern method |
Raschig Group PiMC 1221 High gloss PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 50.0 - 75.0 µm | 50.0 - 75.0 µm | D 0.5, SATP-114, Malvern method |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 50.0 - 75.0 µm | 50.0 - 75.0 µm | D 0.5, SATP-114, Malvern method |
Raschig Group PiMC 1249 Sanitary, mix color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Particle Size | 50.0 - 75.0 µm | 50.0 - 75.0 µm | D 0.5, SATP-114, Malvern method |
Raschig Group PiMC 1253 Highly flame retardant This FR PiMC grade has been developed for top coats over M1 SMC/BMC grades. Such combinations will meet Europe’s most stringent FR tests for interiors of rolling stock, such as BS 476 and Spanish E.. |
|||
Particle Size | 50.0 - 75.0 µm | 50.0 - 75.0 µm | D 0.5, SATP-114, Malvern method |
Raschig Group PiMC 1841 Metallic colors Adding metallic effect pigments to powder coatings gave rise to several application problems such as “spitting”. Synres-Almoco’s Metallic PiMC 1841 ensures easy processing and homogeneous surface.. |
|||
Particle Size | 50.0 - 75.0 µm | 50.0 - 75.0 µm | D 0.5, SATP-114, Malvern method |
Raschig Group PiMC 1949 Granite colors PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |