Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 5.0 µm | >= 5.0 µm | 10% smaller than |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 5.0 µm | 5.0 µm | |
Poco Graphite AXF-5F Biomedical Grade Graphite POCO has developed post synthesis modifications to make our graphites more suitable to specific conditions. As a producer of highly technical, specialty materials, POCO also offers design engineerin.. |
|||
Particle Size | <= 5.0 µm | <= 5.0 µm | |
Poco Graphite EDM-1 EDM Graphite Applications:Fabricating electrodes with good detail Low wear electrodes High detail roughing electrodesMolds and dies |
|||
Particle Size | 5.0 µm | 5.0 µm | 90% of particles less than |
Old Hickory APG-300 Kentucky Ball Clay This is an extremely low 325 Mesh wet residue clay. It can be employed in a variety of applications where high purity mineral filler is required. It has a moderate GE brightness value and is particu.. |
|||
Particle Size | <= 5.0 µm | <= 5.0 µm | 84% of particles less than |
Old Hickory Dunn Tennessee Ball Clay Dunn clay is a selection originating from our Gleason, TN processing facility and is characterized by moderately high levels of kaolin interspersed with the presence of some carbon content. It is an.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 72.3% of particles less than |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 73.3% of particles less than |
Old Hickory M&M Clays, Inc. Wilco-UPF Kaolin Clay Wilco UPF is finer grained kaolin and can be employed in a ceramic formulation where higher permeability type kaolin is not required. It has excellent suspension qualities and lends good film streng.. |
|||
Particle Size | 5.0 - 150 µm | 5.0 - 150 µm | range |
Potters Industries Q-Cel® 5019 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Particle Size | 5.0 - 135 µm | 5.0 - 135 µm | |
Potters Industries Q-Cel® 7023S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 5.0 - 125 µm | 5.0 - 125 µm | |
Potters Industries Q-Cel® 7036 Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 5.0 µm | 5.0 µm | |
Poco Graphite AXF-5Q10W Biomedical Grade Graphite POCO has developed post synthesis modifications to make our graphites more suitable to specific conditions. As a producer of highly technical, specialty materials, POCO also offers design engineerin.. |
|||
Particle Size | <= 5.0 µm | <= 5.0 µm | |
Poco Graphite EDM-C3 EDM Graphite POCO's EDM-C3 is a high quality graphite infiltrated with copper, recommended where speed, wear, and surface finish are important. Unequalled for fragile electrodes, many EDM'ers choose this grade t.. |
|||
Particle Size | 5.0 µm | 5.0 µm | |
Poco Graphite TRA Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Particle Size | 5.0 µm | 5.0 µm | 50% of particles, (MVG Powder) |
Ferro EG 0225 Specialty Glass Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 50% of particles |
Ferro EG 2739 Thick Film Glass Glass Type: Pb-Zn-B Typical Powder Form: MVG Typical Application: Resistor Overglaze Ferro produces standard and custom glass products that are used in thick film compositions including resistors, .. |
|||
Particle Size | <= 5.0 µm | <= 5.0 µm | 79% finer |
Malvern Minerals Novacite® L-337 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 81.5% finer than |
Imerys Allenâ„¢ R Kaolin Allen is an intermediate-grained kaolin suitable for use as a filler in soft rubber products, plastic compounds, adhesives, protective coatings and similar applications.Information provided by Imery.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 79% finer than |
Imerys Ewingâ„¢ Kaolin Ewing is an intermediate grained air-floated kaolin which is selected, processed and controlled to meet specific requirements of the fibreglass industry.Information provided by Imerys |
|||
Particle Size | 5.0 µm | 5.0 µm | 81% finer than |
Imerys KT-Cast/Rogersâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 5.0 - 9.0 µm | 5.0 - 9.0 µm | 10% |
H.C. Starck Amperit® 281 Gas Atomized (NiAl 95-5) |
|||
Particle Size | 5.0 µm | 5.0 µm | 50% of particles |
Ferro EG 2791 Thick Film Glass Glass Type: Bi-Pb-Zn Typical Powder Form: MVG Typical Application: End Termination Ferro produces standard and custom glass products that are used in thick film compositions including resistors, co.. |
|||
Particle Size | 5.0 µm | 5.0 µm | Springback 9.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® GB98/75 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 5.0 µm | 5.0 µm | at a density of 1.81 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® KS44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 5.0 µm | 5.0 µm | Springback 11.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS5-25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 5.0 - 7.0 µm | 5.0 - 7.0 µm | Grain Size; Intercept Method |
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |
|||
Particle Size | 5.0 µm | 5.0 µm | Average Crystal Size - Thin Section Test |
CoorsTek Alumina-Zirconia Composite, AZ-25 Information provided by CoorsTek. |
|||
Particle Size | 5.0 µm | 5.0 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC8 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 5.0 µm | 5.0 µm | D90 |
Dandong Taico Minerals TAICOCITE® TC80 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | <= 5.0 µm | <= 5.0 µm | Fineness of Grind |
Gwent Electronic Materials C2040226D4 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Particle Size | 5.0 µm | 5.0 µm | Loosely agglomerated |
Arkema Group KYNAR® 2501-20 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Very flexible, very soluble. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low p.. |