Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 41 µm | 41 µm | Average Diameter |
Potters Industries Conduct-O-Fil® S3000-S Silver-Coated Solid Glass Spheres Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-a.. |
|||
Particle Size | 41 µm | 41 µm | Average Diameter |
Potters Industries Conduct-O-Fil® S3000-S2M Silver-Coated Solid Glass Spheres Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-a.. |
|||
Particle Size | 41 µm | 41 µm | Average Diameter |
Potters Industries Conduct-O-Fil® S3000-S3M Silver-Coated Solid Glass Spheres Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-a.. |
|||
Particle Size | 41 µm | 41 µm | Average Diameter |
Potters Industries Conduct-O-Fil® SN325P25-LD Silver-coated Nickel Granules Applications:EMI shieldingConductive adhesivesZ-axis conductive filmsAdvantages:Stable at high temperaturesParticles can be magnetically alignedLow density version (LD) has 10% less mass per volumeI.. |
|||
Particle Size | 41 µm | 41 µm | Average Diameter |
Potters Industries Conduct-O-Fil® S3000-S4M Silver-Coated Solid Glass Spheres Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-a.. |