Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 34 µm | 34 µm | Average Diameter |
Potters Industries Conduct-O-Fil® S3000-S2.5N Silver-Coated Solid Glass Spheres Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-a.. |
|||
Particle Size | 34 µm | 34 µm | Average Diameter |
Potters Industries Conduct-O-Fil® S3000-S3N Silver-Coated Solid Glass Spheres Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-a.. |
|||
Particle Size | 34 - 41 µm | 34 - 41 µm | 50% |
H.C. Starck Amperit® 109.066 Agglomerated Sintered Molybdenum (Mo) |
|||
Particle Size | 34 µm | 34 µm | Before Conversion |
Silberline Silvet® 838-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Particle Size | 34 µm | 34 µm | |
Silberline Sparkle Silver® Premier 55 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Particle Size | 34 µm | 34 µm | Before Conversion |
Silberline Sparkle Silvet® Premier 838-30-E1 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final .. |
|||
Particle Size | 34 µm | 34 µm | |
Silberline Sparkle Silvex® Premier 838-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Particle Size | 34 µm | 34 µm | |
Silberline Sparkle Silvex® Premier 838-20-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Particle Size | 34 µm | 34 µm | |
Silberline Tufflake® 2222-AR Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |