Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
Particle Size | 3.0 µm | 3.0 µm | median; Microtrac |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco NYGLOS® MSTPO Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Median Grain Diameter |
Nabaltec NABALOX® NO 315 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | <= 3.0 µm | <= 3.0 µm | Best Grade |
Oceanchem Group Decabromodiphenyl Ethane (DBDPE/8010) Molecular Formula: C14Br10H4Cas No.: 84852-53-9Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: This.. |
|||
Particle Size | <= 3.0 µm | <= 3.0 µm | Best Grade |
Oceanchem Group Decabromodiphenyl Oxide (DECA/DBDPO) Molecular Formula: C12Br10OCas No.: 1163-19-5Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: It is .. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Excellent Grade |
Oceanchem Group Zinc Borate Information Provided by Oceanchem Group |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | D<sub>50</sub> |
NYC YT3X Y2O3 Powder |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles |
Ferro EG 0024 Specialty Glass Glass Type: Si-B-MG-Al Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles |
Ferro EG 2782 Specialty Glass Glass Type: Ca-Si-B Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 3.0 µm | 3.0 µm | d90 |
Magyar Aluminum ALO-EL-7P Alumina Ground Alumina |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | d50 |
Magyar Aluminum Zeolite |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | average |
Malvern Minerals Novacite® L-207A Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | average |
Malvern Minerals Novakup® L-207A Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% |
Minelco UltraCarb LH15C-10 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% |
Minelco UltraCarb LH15X Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | <= 3.0 µm | <= 3.0 µm | Fineness of Grind |
Gwent Electronic Materials C2050425D1 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Particle Size | 3.0 µm | 3.0 µm | Crystal Size |
Momentive Performance Materials HCPH Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powders of grades HCP, HCPH, HCPL, and AC6004 are generally single-crystal hexagonal platelets with very high purity. The mean particle sizes for these ultra-.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles |
Ferro EG 0002 Glazes and Sealants Glass Type: Si-Al-Ba Typical Powder Form: VWG Typical Application: SiC Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulatin.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Median Grain (d50) |
CeramTec Rubalit® 708S Alumina, 96% Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | |
Dow Corning EP-9293 AL Cosmetic Powder A unique combination of a white cross-linked dimethyl polysiloxane elastomer powder and fumed alumina. As with EP-9289 LL, this combination allows the powder to improve flow and reduce agglomeration.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Grain Size |
CoorsTek ACI-Ni10 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
Particle Size | 3.0 µm | 3.0 µm | Median |
CIMBAR Miti-Wite B3 Chemically Purified White Barite (BaSO4) Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes .. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | median, milled |
ATI Wah Chang Hafnium Oxide, HfO2 A free flowing, coarse, tan powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |