Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2.00 - 50.0 µm | 2.00 - 50.0 µm | Average value: 30.4 µm Grade Count:43 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |