Physical Properties Metric English Comments
Particle Size 17 µm
17 µm
median; Microtrac
Nyco M15 WOLLASTOCOAT® Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Particle Size 17 µm
17 µm
Median Diameter
Omya PULPROWHITE® 17 - SA Calcium Carbonate
A dry ground calcium carbonate with a broad particle distribution and closely controlled top size.Information supplied by Omya North America.
Particle Size 17 - 21 µm
17 - 21 µm
10%
H.C. Starck Amperit® 110.2 Agglomerated Sintered (Mo-Mo2C)
Particle Size 17 - 21 µm
17 - 21 µm
10%
H.C. Starck Amperit® 512.074 Agglomerated Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12
Particle Size 17 - 21 µm
17 - 21 µm
10%
H.C. Starck Amperit® 519.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Particle Size 17 - 21 µm
17 - 21 µm
10%
H.C. Starck Amperit® 527.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Particle Size 17 - 22 µm
17 - 22 µm
10%
H.C. Starck Amperit® 554.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 17 - 21 µm
17 - 21 µm
10%
H.C. Starck Amperit® 588.074 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 45/15 µm
Particle Size 17 - 22 µm
17 - 22 µm
10%
H.C. Starck Amperit® 832.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3)
Particle Size 17 - 21 µm
17 - 21 µm
10%
H.C. Starck Amperit® 558.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 17 - 21 µm
17 - 21 µm
10%
H.C. Starck Amperit® 599.074 Agglomerated Sintered Molybdenum Carbide (Cr2O3)
Particle Size 17 µm
17 µm
Silberline A-6205
A-6205 is a standard grade; class B, medium sized, leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance
Particle Size 17 µm
17 µm
Silberline Aquasil® "BP" SO
Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and ..
Particle Size 17 µm
17 µm
Before Conversion
Silberline Aquavet® 251-136M
Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly..
Particle Size 17 µm
17 µm
Silberline EternaBrite® Premier 251
EternaBrite® Premier 251 is a fine, very bright, leafing aluminum pigment with excellent opacity and distinctness of image (D.O.I) for solvent based general industrial coatings. This grade is not..
Particle Size 17 µm
17 µm
Silberline EternaBrite® Premier 251-DL
EternaBrite® Premier "DL" pigments are leafing aluminum pigment pastes carried in a glycol. These grades are based on cornflake geometry and offer enhanced leafing properties flexographic and gra..
Particle Size 17 µm
17 µm
Silberline EternaBrite® Premier 251-PA
EternaBrite® Premier pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced leafing properties in solven..
Particle Size 17 µm
17 µm
Silberline Sil-O-Wet® 2052NL-PA
Sil-O-Wet® grades are leafing and non-leafing aluminum pigment pastes carried in isopropyl alcohol in which the aluminum flakes have been chemically treated to reduce the aluminum-water reaction...
Particle Size 17 µm
17 µm
Silberline SparkleBriteâ„¢ 190NL-DL
SparkleBriteâ„¢ "DL" pigments are non-leafing aluminum pigment pastes carried in a glycol. These grades are based on cornflake geometry and produce strong metallic effects in flexographic and gra..
Particle Size 17 µm
17 µm
Silberline Sparkle Silver Ultraâ„¢ 6555
Sparkle Silver Ultraâ„¢ grades are very bright lenticular automotive aluminum pigments. They offer a very smooth patina and narrow particle size distribution, allowing the formulator to create ve..
Particle Size 17 µm
17 µm
Silberline SparkleBriteâ„¢ Premier 2052NL-PA
SparkleBriteâ„¢ Premier pigments are non-leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced metallic effects in s..
Particle Size 17 µm
17 µm
Silberline Stamford "O" Standard Series
Stamford O is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This is an economical grade with cornflake geometry and wide particle size distribution ra..
Particle Size 17 µm
17 µm
Silberline Tufflake® 3120-AR
Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app..
Particle Size 17 µm
17 µm
d90, Typical
TIMCAL TIMREX® C-LUB 306 Primary Synthetic Graphite
Information provided by TIMCAL
Particle Size 17 µm
17 µm
d90
TIMCAL TIMREX® MX15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 17 - 23 µm
17 - 23 µm
Average; ATO 40-41-0 (Coulter Counter)
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6
Information provided by Arkema Group
Particle Size 17 - 23 µm
17 - 23 µm
Average; ATO 40-41-0 (Coulter Counter)
Arkema Group ORGASOL® 3202 D Nat 1 Copolyamide 6/12
Information provided by Arkema Group
Particle Size 17 µm
17 µm
Median
CIMBAR BARIMITE™ G-50 High Purity Barite (BaSO4)
Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemi..
Particle Size 17 - 21 µm
17 - 21 µm
10%
H.C. Starck Amperit® 529.074 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo)
Particle Size 17 - 21 µm
17 - 21 µm
10%
H.C. Starck Amperit® 551.074 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)