Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 10 µm | >= 10 µm | 10% smaller than |
Nyco NYAD® M100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 10 µm | 10 µm | |
Poco Graphite EDM-200 EDM Graphite POCO's EDM-200 is an isotropic Superfine particle graphite providing good strength, surface finish, and wear resistance.Applications:Structural ribsRoughing or finishing electrodesLarge featured mol.. |
|||
Particle Size | 10 µm | 10 µm | 87.7% of particles less than |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals 4140 Low Alloy Steel Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals 420 Stainless Steel Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals H13 Tool Steel Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | <= 10 µm | <= 10 µm | SRRG Powder |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 10 µm | <= 10 µm | SRRG Powder |
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | d50 |
Magyar Aluminum ALOLT 8AF Aluminum Hydroxide Ground type |
|||
Particle Size | <= 10 µm | <= 10 µm | 69% finer |
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | >= 10 µm | >= 10 µm | 20% finer |
Malvern Minerals Novakup® 325 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 10 µm | 10 µm | 99% finer than |
Imerys Bardenâ„¢ Kaolin Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys |
|||
Particle Size | 10 µm | 10 µm | 93% finer than |
Imerys Diamondâ„¢ Kaolin Diamond is an intermediate-grained montmorillonitc kaolin used primarily in plastic formed bodies. This kaolin is known for its good strength and white-firing characteristics.Information provided by.. |
|||
Particle Size | 10 µm | 10 µm | 91% finer than |
Imerys Ewingâ„¢ Kaolin Ewing is an intermediate grained air-floated kaolin which is selected, processed and controlled to meet specific requirements of the fibreglass industry.Information provided by Imerys |
|||
Particle Size | 10 µm | 10 µm | Average Particle Diameter |
Mitsui UNISTOLEâ„¢ R-120K Polyolefinic Primer/ Adhesive UNISTOLEâ„¢ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristi.. |
|||
Particle Size | 10 µm | 10 µm | Maximum of 5% less than |
H.C. Starck Amperit® 849.054 Sintered Yttria (Y2O3) |
|||
Particle Size | 10 µm | 10 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 615 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 10 - 210 µm | 10 - 210 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ CG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Particle Size | 10 - 500 µm | 10 - 500 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ SG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Particle Size | 10 - 150 µm | 10 - 150 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-150 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-150 are white aluminosilicate multicellular hollow spheres. The density of this product is 0.30 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-150 hollo.. |
|||
Particle Size | 10 - 210 µm | 10 - 210 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-200 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-200 are white aluminosilicate multicellular hollow spheres. The density of this product averages 0.25 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-200.. |
|||
Particle Size | 10 µm | 10 µm | |
Silberline Aquavexâ„¢ 301-207S Aquavexâ„¢ grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary no.. |
|||
Particle Size | 10 µm | 10 µm | d50 |
TIMCAL TIMREX® PG25 Natural P/M Special-Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | <= 10 µm | <= 10 µm | |
Epoxy Technology EPO-TEK® OG133-8 UV Cure Optical Epoxy Material Description: A single component, UV curable, thixotropic flexible epoxy adhesive/encapsulant designed for semiconductor and opto-electronic packaging. Glob top over IC and wire bonds, and .. |
|||
Particle Size | 10 - 16 µm | 10 - 16 µm | D(0.5) |
Akzo Nobel Expancel® 820 SL 40 Unexpanded microspheres in aqueous dispersion Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | <= 10 µm | <= 10 µm | 90% smaller than |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 10 - 500 µm | 10 - 500 µm | |
Solvay MIRAPOL® SURF-S PFREE POWER Surfactant Description: Blend of acrylic based polymer and sodium carbonate. This polymer is used as a rinse-aid agent to replace the nonionic surfactant 3-in-1 product in automatic dish wash. It is very effic.. |
|||
Particle Size | 10 µm | 10 µm | Average Particle Diameter |
Mitsui UNISTOLE™ R-200 Polyolefinic Primer/ Adhesive UNISTOLE™ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristics E.. |
|||
Particle Size | 10 - 16 µm | 10 - 16 µm | D(0.5) |
Akzo Nobel Expancel® 054 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 10 - 16 µm | 10 - 16 µm | 50% of particles, (TF Powder) |
Ferro CF 7575 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci.. |