Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 3.80 - 3.95 g/cc | 0.137 - 0.143 lb/in³ | |
China-Yixing Longly Refractories 99 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |