Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.40 - 1.60 g/cc | 0.0506 - 0.0578 lb/in³ | JIS K5101 |
NYC YT3WBHQ Y2O3 Powder for Spray Coating High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.Narrow particle size distributionTailorable for each spray coating technologyNo c.. |
|||
Bulk Density | 1.50 - 1.60 g/cc | 0.0542 - 0.0578 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 145 Refractory Insulating Castable Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also avail.. |
|||
Bulk Density | 0.300 - 1.60 g/cc | 0.0108 - 0.0578 lb/in³ | |
GrafTech GRAFCELL® GDB Graphite Gas Diffusion Barrier GRAFCELL® Gas Diffusion Barrier (GDB) material is a thin, perforated structure made from a continuous matrix of expanded natural graphite with excellent electrical conductivity, thermal conductiv.. |
|||
Bulk Density | 1.00 - 1.60 g/cc | 0.0361 - 0.0578 lb/in³ | loose |
Solvay Chemicals Strontium carbonate coarse powder Strontium carbonate coarse powder is used in the production of glazes, frits and for production of strontium pigments. Another application for strontium carbonate coarse powder is the production of .. |
|||
Bulk Density | 1.51 - 1.60 g/cc | 0.0546 - 0.0578 lb/in³ | |
3M #11 Roofing Granule (Wausau) 3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre.. |
|||
Bulk Density | 1.51 - 1.60 g/cc | 0.0546 - 0.0578 lb/in³ | |
3M Cool Roofing Granule (Wausau) 3M Cool Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products are designed specifically to have a higher total solar reflectance than standard granules... |
|||
Bulk Density | 1.47 - 1.60 g/cc | 0.0531 - 0.0578 lb/in³ | |
3M Headlap Roofing Granule (Wausau) 3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He.. |
|||
Bulk Density | 1.50 - 1.60 g/cc | 0.0542 - 0.0578 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Bulk Density | 1.50 - 1.60 g/cc | 0.0542 - 0.0578 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere... |