Physical Properties Metric English Comments
Bulk Density 1.40 - 1.50 g/cc
0.0506 - 0.0542 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable
Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p..
Bulk Density 1.40 - 1.50 g/cc
0.0506 - 0.0542 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable
Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al..
Bulk Density 1.40 - 1.50 g/cc
0.0506 - 0.0542 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable